Embodiment 1
[0015] A method for pretreatment of the surface of a chemical pump pump body before painting, comprising the following steps:
[0016] a. Remove the surface rust of the chemical pump to be painted until there is no visible rust on the surface;
[0017] b. Use clarified lime water to evenly spray the surface of the chemical pump after the rust removal above at a pressure of 1.5 MPa. After spraying evenly for 10 minutes, adjust the pressure to 1.0 MPa and continue spraying evenly for 10 minutes, then let it stand for 20 minutes, and then use boiling water. Carry out a surface rinsing, after rinsing, use a hot air blower to dry the surface moisture;
[0018] c Prepare the treatment agent A and heat it to 55°C. Use a brush to directly paint the treatment agent A on the surface of the chemical pump. After standing for 30 minutes, rinse it with boiling water, and then wipe the surface of the chemical pump with a dry cloth. Clean; the treatment agent A is made of the following ingre...
Embodiment 2
[0024] A method for pretreatment of the surface of a chemical pump pump body before painting, comprising the following steps:
[0025] a. Remove the surface rust of the chemical pump to be painted until there is no visible rust on the surface;
[0026] b. Use clarified lime water to evenly spray the surface of the chemical pump after the rust removal above at a pressure of 1.5 MPa. After spraying evenly for 10 minutes, adjust the pressure to 1.0 MPa and continue spraying evenly for 10 minutes, then let it stand for 20 minutes, and then use boiling water. Carry out a surface rinsing, after rinsing, use a hot air blower to dry the surface moisture;
[0027] c Prepare the treatment agent A and heat it to 55°C. Use a brush to directly paint the treatment agent A on the surface of the chemical pump. After standing for 30 minutes, rinse it with boiling water, and then wipe the surface of the chemical pump with a dry cloth. Clean; the treatment agent A is made of the following ingre...
Embodiment 3
[0033] A method for pretreatment of the surface of a chemical pump pump body before painting, comprising the following steps:
[0034] a. Remove the surface rust of the chemical pump to be painted until there is no visible rust on the surface;
[0035] b. Use clarified lime water to evenly spray the surface of the chemical pump after the rust removal above at a pressure of 1.5 MPa. After spraying evenly for 10 minutes, adjust the pressure to 1.0 MPa and continue spraying evenly for 10 minutes, then let it stand for 20 minutes, and then use boiling water. Carry out a surface rinsing, after rinsing, use a hot air blower to dry the surface moisture;
[0036] c Prepare the treatment agent A and heat it to 55°C. Use a brush to directly paint the treatment agent A on the surface of the chemical pump. After standing for 30 minutes, rinse it with boiling water, and then wipe the surface of the chemical pump with a dry cloth. Clean; the treatment agent A is made of the following ingre...