Production technology of color-changing leather

A production process and leather technology, applied in the field of production process of color-changing leather, can solve the problems of short reversible life of discoloration and poor discoloration effect, and achieve long reversible life of discoloration, prolong discoloration life and good discoloration effect

Inactive Publication Date: 2017-06-13
福建省永建皮革科技股份有限公司
View PDF5 Cites 3 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

The research on the production process of photosensitive and temperature-sensitive reversible discoloration leather is also one of the hot spots in the leather industry. At present, this kind of discoloration leather has problems such as poor discoloration effect and short reversible life of discoloration.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0026] A production process of color-changing leather, comprising the following steps:

[0027] (1) Prepare color-changing paste, which contains the following raw materials in parts by weight: 100 parts of composite resin 8F8080, 30 parts of solvent MEK, 4 parts of 3626 organic yellow dye, 1 part of hand feeling agent SG-01, color-changing agent BS- 01 3 parts, mix the above raw materials evenly;

[0028] (2) Evenly coat the discoloration slurry prepared in step (1) on the release paper with a coating thickness of 20 μm, and dry at 120° C. for 10 minutes to form a discoloration layer;

[0029] (3) Evenly coat the adhesive 2062 primer resin on the dried discoloration layer obtained in step (2), the coating thickness is 20 μm, and dry at 120° C. for 8 minutes;

[0030] (4) At 80°C, the release paper coated with the color-changing slurry and the adhesive in sequence is bonded to the leather as the skin base, and the side of the release paper coated with the adhesive is pressed t...

Embodiment 2

[0034] A production process of color-changing leather, comprising the following steps:

[0035] (1) Prepare color-changing slurry, which contains the following raw materials by weight: 100 parts of composite resin 8F8080, 25 parts of solvent MEK, 5 parts of 3626 organic yellow dye, 2 parts of hand feeling agent SG-01, color-changing agent BS- 01 4 parts, mix the above raw materials evenly;

[0036] (2) Evenly coat the color-changing paste prepared in step (1) on the release paper with a coating thickness of 22 μm, and dry at 130° C. for 8 minutes to form a color-changing layer;

[0037] (3) Apply adhesive 2062 primer resin evenly on the dried discoloration layer obtained in step (2), the coating thickness is 22 μm, and dry at 130° C. for 8 minutes;

[0038] (4) At 90°C, the release paper coated with the color-changing paste and the adhesive in sequence is bonded to the leather as the skin base, and the side of the release paper coated with the adhesive is pressed together wit...

Embodiment 3

[0042] (1) Prepare color-changing slurry, which contains the following raw materials in parts by weight: 100 parts of composite resin 8F8080, 20 parts of solvent MEK, 4 parts of 6637 brown dye, 3 parts of hand feeling agent SG-02, color-changing agent BS-01 5 parts, mix the above raw materials evenly;

[0043] (2) Evenly coat the color-changing paste prepared in step (1) on the release paper with a coating thickness of 25 μm, and dry at 140° C. for 5 minutes to form a color-changing layer;

[0044] (3) Evenly coat the adhesive 2062 primer resin on the dried discoloration layer obtained in step (2), the coating thickness is 25 μm, and dry at 140° C. for 5 minutes;

[0045] (4) At 100°C, the release paper coated with the color-changing paste and the adhesive in turn is bonded to the leather as the skin base, and the adhesive is applied to the side of the release paper with a pressure of 100kg. on the leather, and then tear off the release paper to get a semi-finished product of...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a production process of discolored leather. The prepared discoloration slurry is uniformly coated on release paper to form a discolored layer, and then an adhesive is uniformly coated on the dried discolored layer, and then the layers are sequentially coated The release paper with discolored pulp and adhesive is attached to the leather as the leather blank, and the adhesive-coated side of the release paper is pressed onto the leather with a pressure of 80-100kg, and then the release paper is torn off. paper to obtain the semi-finished product of the color-changing leather; finally, the color-changing layer of the obtained semi-finished product is covered with a layer of high-temperature resistant oil paper, and rolled to obtain the color-changing leather. The invention provides a production process for discolored leather, and the produced discolored leather has the characteristics of good discoloration effect and long discoloration reversibility life.

Description

technical field [0001] The invention relates to the technical production field of leather, in particular to a production process of discoloration leather. Background technique [0002] Color-changing leather usually refers to artificial leather that changes color under changes in temperature or pressure. Stress-changing leather is one of the representatives of color-changing leather. The deformed part will show a color change, and with the change of the deformation gradient, the color will show a gradual change from light to dark, which can give people a natural and soft feeling. Once the external force is removed, the color of the leather will naturally return to its original state. The research on the production process of photosensitive and temperature-sensitive reversible discoloration leather is also one of the hotspots in the leather industry. At present, this kind of discoloration leather has problems such as poor discoloration effect and short reversible life of dis...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): B32B9/02B32B9/06B32B7/12B32B38/14B32B37/12D06N3/00
CPCB32B9/025B32B7/12B32B9/06B32B37/12B32B38/145D06N3/0065D06N3/0097D06N2209/0823D06N2209/1642D06N2211/28
Inventor 陈惜治林树生陈浩
Owner 福建省永建皮革科技股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products