An internal stress and sand box technology, applied in manufacturing tools, furnaces, heat treatment equipment, etc., can solve the problems affecting the gap between the upper and lower sand boxes, residual internal stress, and wall warping, etc., to eliminate residual internal stress, easy to Mastery, low-cost effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0009] The present invention is a simple method for eliminating the internal stress of the casting sand box, which is carried out according to the following steps:
[0010] S1: Divide each wall plate of the casting flask into several sections symmetrical along the center line;
[0011] S2: Use two sets of heat guns to heat one of the wall panels from the center line to both sides at the same time, the heating temperature is controlled at 600-650 ° C, and the heating time is 8-10 hours;
[0012] S3: measure the tilting angle of the upper surface of the wallboard;
[0013] S4: If the tilting angle of the upper surface of the panel meets the accuracy requirements, start to process another panel according to S2, and if it does not meet the requirements, repeat the heating of the panel. The heating sequence is also to heat from the center line to both sides at the same time. The heating time is 2h.
[0014] The method provided by the invention can eliminate the residual internal ...