Plate bending method
A sheet and bending technology, applied in the field of sheet bending, can solve the problems of breakage, unfavorable operation, bad deformation, etc., and achieve the effect of reducing springback rate, improving quality, and simple steps.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] A method for bending a plate, comprising the steps of:
[0029] S1: Select wood
[0030] Place the wood to be processed on the cutting machine for cutting, and specifically cut it into a straight plate with a thickness of 2 cm;
[0031] S2: Washing and boiling
[0032] Put the cut plate into the cleaning pool for cleaning, and put the cleaned plate into the boiling pool for 20 minutes of boiling;
[0033] S3: cooling, softening
[0034] Take out the boiled plate, and cool it to 26 degrees Celsius under the cooling of natural wind, put the cooled plate into the softening liquid in the softening tank for continuous softening for 10 days;
[0035] S4: Second cleaning and drying
[0036] After the softened plate is taken out, it is placed in the secondary cleaning tank for 2 minutes of cleaning. After cleaning, the plate is placed in a drying oven for drying, and the plate is taken out when the moisture content of the plate is 18%.
[0037] S5: bending, initial shape ...
Embodiment 2
[0048] A method for bending a plate, comprising the steps of:
[0049] S1: Select wood
[0050] Place the wood to be processed on the cutting machine for cutting, and specifically cut it into a straight plate with a thickness of 4 cm;
[0051] S2: Washing and boiling
[0052] Put the cut plate into the cleaning pool for cleaning, and put the cleaned plate into the boiling pool for 30 minutes of boiling;
[0053] S3: cooling, softening
[0054] Take out the boiled plate, and cool it to 28 degrees Celsius under the cooling of natural wind, put the cooled plate into the softening liquid in the softening tank for continuous softening for 12 days;
[0055] S4: Second cleaning and drying
[0056] After the softened plate is taken out, it is placed in the secondary cleaning tank for 3 minutes of cleaning. After cleaning, the plate is placed in a drying oven for drying, and the plate is taken out when the moisture content of the plate is 23%.
[0057] S5: bending, initial shape ...
Embodiment 3
[0068] A method for bending a plate, comprising the steps of:
[0069] S1: Select wood
[0070] Place the wood to be processed on the cutting machine for cutting, and specifically cut it into a straight plate with a thickness of 6 cm;
[0071] S2: Washing and boiling
[0072] Put the cut plate into the cleaning pool for cleaning, and put the cleaned plate into the boiling pool for 40 minutes of boiling;
[0073] S3: cooling, softening
[0074] Take out the boiled plate, and cool it to 30 degrees Celsius under the cooling of natural wind, put the cooled plate into the softening liquid in the softening tank for continuous softening for 14 days;
[0075] S4: Second cleaning and drying
[0076] After the softened plate is taken out, it is placed in the secondary cleaning tank for 4 minutes of cleaning. After cleaning, the plate is placed in a drying oven for drying, and the plate is taken out when the moisture content of the plate is 18-28%. ;
[0077] S5: bending, initial s...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com