Embodiment 1
[0035] By mixing 50g of neodymium particles with an average diameter of 0.5μm, 250g of silicon carbide particles with an average diameter of 35μm, 100g of alumina particles with an average diameter of 25μm, 10g of amethyst powder with an average diameter of 35μm, and 50g of germanium particles with an average diameter of 80μm and 50 g of vein porphyry particles with an average diameter of 75 μm to prepare a soot reducing composition.
[0036] The soot reducing composition was mixed with 1 liter of alkaline ionized water to prepare a soot reducing composition dispersion, which was then irradiated with ultrasonic waves for 20 minutes to uniformly disperse.
Embodiment 2
[0038] Prepared in the same manner as in Example 1, instead of 350 g of silicon carbide particles and 100 g of alumina particles, 300 g of silicon carbide particles and 50 g of alumina particles were mixed to prepare a soot reducing composition dispersion.
Embodiment 3
[0040] Prepared in the same manner as in Example 1, a soot reducing composition dispersion was prepared by adding 300 g of neodymium particles instead of 50 g.