Unlock instant, AI-driven research and patent intelligence for your innovation.

A kind of production method of the button battery that reduces false soldering rate and button battery made

A technology of button battery and production method, which is applied in the manufacture of cylindrical shell battery/battery, primary battery, secondary battery, etc., can solve the problem of high defective rate of button battery, falling off of the first output conductor, welding strength detection, etc. problem, to achieve the effect of eliminating short circuit phenomenon, reducing virtual welding rate and improving yield rate

Active Publication Date: 2021-01-15
FUJIAN NANPING YANPING DISTRICT NANFU NEW ENERGY TECH CO LTD
View PDF13 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Since there is a risk of virtual welding in both resistance welding and laser welding, and the welding operation between the first output conductor and the first pole shell in the prior art is carried out after the electric core is loaded into the first pole shell, it cannot The welding strength is detected in time, which leads to a high defect rate of button batteries; in addition, in the prior art, the first output conductor usually extends to the axial cavity area of ​​the battery core, and in this area is connected to the first pole The shells are welded and fixed to realize electrical connection. However, since the cell will expand radially after absorbing the electrolyte, the expansion of the cell will drive the first output conductor to move radially, which will easily lead to the breakage of the solder joint and the first output conductor from The first pole shell falls off, and the welding spot position of the first output conductor is usually a conductive area. Risk of short circuit due to pole piece contact

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • A kind of production method of the button battery that reduces false soldering rate and button battery made
  • A kind of production method of the button battery that reduces false soldering rate and button battery made
  • A kind of production method of the button battery that reduces false soldering rate and button battery made

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0026] combine Figure 1~Figure 3 , a button battery production method that reduces the false welding rate, the button battery includes a positive electrode case 11, a negative electrode case 12 and a battery cell 30, the positive electrode case 11 and the negative electrode case 12 are cup-shaped, and the battery cell 30 is mainly It is formed by winding a positive electrode sheet 31, a negative electrode sheet 32, and a diaphragm 33. An axial cavity 34 is formed in the center of the battery core 30. The positive electrode sheet 31 is electrically connected to a positive electrode tab 21. The negative electrode sheet 32 Electrically connected with a negative electrode tab 22, the positive electrode casing 11 and the negative electrode casing 12 are cup-shaped, the negative electrode casing 12 is used as the bottom casing, and the positive electrode casing 11 is used as the top casing, and the production method of the button cell comprises the following steps:

[0027] S1: Pre...

Embodiment 2

[0035] Such as Figure 4 As shown, a button cell production method that reduces the false soldering rate is different from the button cell production method that reduces the false soldering rate in Example 1 in that: the tab 21 with the same polarity as the top case 11 is connected to the top case 11 are electrically connected through conductive glue.

[0036] According to the production method of the button battery that reduces the false soldering rate of Example 2, the button battery is produced. The button battery is different from the button battery of Example 1 in that: the positive electrode tab 21 is glued and fixed in the positive electrode shell 11 through the conductive adhesive layer 100. On the surface.

[0037] Of course, the present invention is not limited to the negative electrode case as the bottom case, it may also be: the positive electrode case is used as the bottom case, and the negative electrode case is used as the top case. In addition, when one of th...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention provides a button battery production method and the button battery produced by reducing the false soldering rate. The button battery production method includes the following steps: first pressing the tab with the same polarity as that of the bottom case against the inner surface of the bottom case Afterwards, the lug is welded on the inner surface of the bottom case, and a first welding spot is formed between the tab and the bottom case, and the first welding point is located on the bottom case outside the vertical projection area of ​​the axial cavity of the battery core on the inner bottom surface; then, put the battery cell into the bottom case; then, set the top case cover on the top of the bottom case, and the upper and lower openings of the top case and the bottom case are oppositely buckled to form a cylindrical button battery shell to accommodate the cell Inside, the tab with the same polarity as the top case is electrically connected to the top case. The use of the production method makes it easy to detect the welding strength between the tab and the corresponding pole shell, thereby reducing the false welding rate of the button battery and finally reducing the product defective rate.

Description

technical field [0001] The invention relates to a production method of a button battery which reduces the false soldering rate and the button battery produced. Background technique [0002] Button cell (button cell), also known as button cell, refers to a battery that looks like a small button. Generally speaking, it has a larger diameter and a thinner thickness (compared to cylindrical batteries such as No. 5 AA batteries on the market), Button batteries are classified from the shape, and the corresponding battery classifications include cylindrical batteries, square batteries, special-shaped batteries, etc. [0003] Button batteries include laminated and wound ones. The basic structure of the wound button battery is: including the first pole shell, the second pole shell, the insulating sealing ring and the battery core, the first pole shell and the second pole shell are oppositely buckled to form a cylindrical button battery shell; There is a gap between the first pole s...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): H01M50/216H01M50/204H01M50/183H01M6/00H01M6/10H01M10/04B23K11/00H01M50/528H01M50/109H01M50/536H01M50/586
CPCH01M6/005H01M6/10H01M10/0427B23K11/00H01M50/216H01M50/183H01M50/528H01M50/531Y02E60/10Y02P70/50
Inventor 常海涛叶永锋张志明苏盛
Owner FUJIAN NANPING YANPING DISTRICT NANFU NEW ENERGY TECH CO LTD