[0032] An HDMI high-definition data cable of the present embodiment includes the following raw materials by weight:
[0033] Mn 0.2%, Ni 0.2%, Si 0.1%, Sn 1.2%, dispersing accelerator 5%, toughness modifier 1%, and the balance is copper;
[0034] The preparation method of the dispersing agent is:
[0035] S1: Preparation of nanomedia: 30 parts of bismuth nitrate, 5 parts of sodium molybdate dihydrate and 2 parts of cetyltrimethylammonium chloride were added to a solution of 35 parts of deionized water, then nitric acid was added to adjust the pH to 4.0 , then the raw materials are jointly transferred into the reactor, and the reaction temperature is 125 ° C to obtain the nanometer medium liquid;
[0036] S2: Preparation of Dispersed Particles: The silicon dioxide and the activation solution are mixed according to the weight ratio of 1:5 to prepare a silicon dioxide dispersion liquid, and then the silicon dioxide dispersion liquid is sent into 20 parts of titanium dioxide powd...
Embodiment 2
[0051] An HDMI high-definition data cable of the present embodiment includes the following raw materials by weight:
[0052] Mn 0.6%, Ni 0.4%, Si 0.4%, Sn 1.5%, dispersing agent 10%, toughness modifier 5%, and the balance is copper;
[0053] The preparation method of the dispersing agent is:
[0054] S1: Preparation of nanomedia: 40 parts of bismuth nitrate, 10 parts of sodium molybdate dihydrate and 8 parts of cetyltrimethylammonium chloride were added to a solution of 45 parts of deionized water, then nitric acid was added to adjust the pH to 5.0 , then the raw materials are jointly transferred into the reactor, and the reaction temperature is 135 ° C to obtain the nanometer medium liquid;
[0055] S2: Preparation of Dispersed Particles: The silica and the activation solution are mixed according to the weight ratio of 1:5 to prepare a silica dispersion, and then the silica dispersion is sent into 30 parts of titanium dioxide powder, and the proton Irradiation, the irradiat...
Embodiment 3
[0070] An HDMI high-definition data cable of the present embodiment includes the following raw materials by weight:
[0071] Mn 0.4%, Ni 0.3%, Si 0.25%, Sn 1.35%, dispersing agent 7.5%, toughness modifier 3%, and the balance is copper;
[0072] The preparation method of the dispersing agent is:
[0073] S1: Preparation of nanomedia: 35 parts of bismuth nitrate, 7.5 parts of sodium molybdate dihydrate and 5 parts of cetyltrimethylammonium chloride were added to a solution of 40 parts of deionized water, then nitric acid was added to adjust the pH to 4.5 , then the raw materials are jointly transferred to the reactor, and the reaction temperature is 130 ° C to obtain the nanometer medium liquid;
[0074] S2: Preparation of Dispersed Particles: The silica and the activation solution are mixed according to the weight ratio of 1:5 to prepare a silica dispersion, and then the silica dispersion is fed into 25 parts of titanium dioxide powder, and the proton Irradiation, the irradia...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com