A crop and coating technology, applied in botany equipment and methods, layered/coated fertilizers, chemicals for biological control, etc., can solve the problem of destroying soil ecological balance, unfriendly soil environment, coating thixotropy To achieve the effect of promoting synthesis and operation, accelerating lignin formation, and improving cold resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Example Embodiment
[0037]Example 1
[0038]Crops coating fertilizer, including the following raw materials: Spirotetramat 8kg, Chlorantraniliprole 8kg, Pyraclostrobin 15kg, Prothioconazole 15kg, Urea 50kg, Potassium Dihydrogen Phosphate 30kg, Boric Acid 5kg, Bentonite 20kg, polyacrylamide 20kg and starch 10kg;
[0039]The preparation method of crop coating medicinal fertilizer specifically includes the following steps:
[0040](1) Weigh the raw materials according to the weight of the above-mentioned crop coating fertilizer;
[0041](2) Add Spirotetramat, Chlorantraniliprole, Pyraclostrobin and Prothioconazole into the mixer, mix and stir for 10 minutes at a speed of 200r / min to obtain material A;
[0042](3) Add material A, urea, potassium dihydrogen phosphate and trace element growth regulator into the mixer, add water to a water content of 40%, mix and stir for 20 minutes at a speed of 100r / min, then add to the granulator to granulate, and then add The dryer is dried, the inlet temperature of the dryer is 200°C, ...
Example Embodiment
[0044]Example 2
[0045]Crops coating fertilizer, including raw materials of the following weights: Spirotetramat 12kg, Chlorantraniliprole 12kg, Pyraclostrobin 20kg, Prothioconazole 20kg, Urea 70kg, Potassium Dihydrogen Phosphate 40kg, Zinc Sulfate 10kg , Attapulgite 30kg, butyl acrylate 30kg and polyvinyl alcohol 20kg;
[0046]The preparation method of crop coating medicinal fertilizer specifically includes the following steps:
[0047](1) Weigh the raw materials according to the weight of the above-mentioned crop coating fertilizer;
[0048](2) Add Spirotetramat, Chlorantraniliprole, Pyraclostrobin and Prothioconazole into the mixer, mix and stir for 20 minutes at a speed of 300r / min to obtain material A;
[0049](3) Add material A, urea, potassium dihydrogen phosphate and trace element growth regulator into the mixer, add water to 50% water content, mix and stir for 30 minutes at a speed of 200r / min, then add to the granulator to granulate, and then add The dryer is dried, the inlet temperatur...
Example Embodiment
[0051]Example 3
[0052]Crops coating fertilizer, including raw materials of the following weights: Spirotetramat 10kg, Chlorantraniliprole 10kg, Pyraclostrobin 18kg, Prothioconazole 18kg, Urea 60kg, Potassium Dihydrogen Phosphate 35kg, Copper Sulfate 8kg , 25kg of sepiolite, 25kg of chitosan and 15kg of gum arabic;
[0053]The preparation method of crop coating medicinal fertilizer specifically includes the following steps:
[0054](1) Weigh the raw materials according to the weight of the above-mentioned crop coating fertilizer;
[0055](2) Add spirotetramat, chlorantraniliprole, pyraclostrobin and prothioconazole into the mixer, mix and stir for 15 minutes at a speed of 250r / min to obtain material A;
[0056](3) Add material A, urea, potassium dihydrogen phosphate and trace element growth regulator into the mixer, add water to 45% water content, mix and stir at a speed of 150r / min for 25min, then add to the granulator to granulate, and then add The dryer is dried, the inlet temperature of the d...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap