A technology of down jacket fabrics and wear-resistant coatings, which is applied in the field of down jackets, can solve the problems of easy damage of the surface wear-resistant layer, poor wear-resistant effect, and shedding, and achieve outstanding bending and wear resistance, excellent wear-resistant effect, and good antibacterial properties sexual effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] A method for preparing a wear-resistant and wrinkle-resistant down jacket fabric, the steps comprising:
[0021] (1) Cotton fiber and bamboo fiber are mixed according to the mass ratio of 1:2, and then interweaved through warp yarn and weft yarn to form primary material;
[0022] (2) Put the primary material into the antibacterial solution and soak for 12h, rinse with clear water after soaking, the antibacterial solution is made by mixing 10wt% chitin, 20wt% Artemisia argyi extract, 20wt% kasone and 50wt% deionized water become;
[0023] (3) Coating wear-resistant paint on the outer surface of the primary material, after the wear-resistant coating is cured, place the primary material in a kneading mill for rolling, and repeat the operations of coating, curing and rolling three times, the first The thickness of the wear-resistant coating is 15nm for the first coating, and the kneading speed after curing is 80r / min, and the kneading time is 6min; the thickness of the sec...
Embodiment 2
[0025] A method for preparing a wear-resistant and wrinkle-resistant down jacket fabric, the steps comprising:
[0026] (1) Mix cotton fiber and bamboo fiber according to the mass ratio of 1:1, and then interweave through warp yarn and weft yarn to form primary material;
[0027] (2) Put the primary material into the antibacterial solution and soak for 18h, rinse with clear water after soaking, the antibacterial solution is made by mixing 30wt% chitin, 10wt% mugwort leaf extract, 15wt% kasone and 45wt% deionized water become;
[0028] (3) Coating wear-resistant paint on the outer surface of the primary material, after the wear-resistant coating is cured, place the primary material in a kneading mill for rolling, and repeat the operations of coating, curing and rolling three times, the first The thickness of the wear-resistant coating for the first coating is 18nm, and the kneading speed after curing is 90r / min, and the kneading time is 7min; the thickness of the second coatin...
Embodiment 3
[0030] A method for preparing a wear-resistant and wrinkle-resistant down jacket fabric, the steps comprising:
[0031] (1) Cotton fiber and bamboo fiber are mixed according to the mass ratio of 2:1, then through warp yarn, weft yarn interweaving, form primary material;
[0032] (2) Put the primary material into the antibacterial solution and soak for 24 hours, rinse with clear water after soaking, the antibacterial solution is made by mixing 20wt% chitin, 20wt% mugwort leaf extract, 20wt% kasone and 40wt% deionized water become;
[0033] (3) Coating wear-resistant paint on the outer surface of the primary material, after the wear-resistant coating is cured, place the primary material in a kneading mill for rolling, and repeat the operations of coating, curing and rolling three times, the first The thickness of the first coating wear-resistant coating is 20nm, and the kneading speed after curing is 100r / min, and the kneading time is 8min; the thickness of the second coating o...