Sunscreen spray and preparation method thereof
A spray and antiseptic technology, applied in the field of sunscreen spray and its preparation, can solve the problems of heavy skin feeling, sticky, high viscosity, etc., and achieve the effect of refreshing skin feeling, preventing contact, and low viscosity
Patent Information
- Authority / Receiving Office
- CN · China
- Current Assignee / Owner
- Publication Date
- 2021-04-09
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure 1 
Figure 2
Abstract
Description
technical field
[0001] The invention relates to the technical field of cosmetics, in particular to a sunscreen spray and a preparation method thereof. Background technique
[0002] Appropriate light can promote the body's metabolism and strengthen people's system. At the same time, appropriate ultraviolet radiation can also sterilize and convert deoxysterol in the skin into vitamin D, which is beneficial to the body's absorption of minerals. However, excessive ultraviolet radiation can , will cause damage to the skin of the human body; among them, long-wave ultraviolet rays will accelerate the formation of melanin and skin aging, and medium-wave ultraviolet rays will cause accounting or protein denaturation in epidermal cells, resulting in skin inflammation and redness. With the improvement of living standards and the gradual strengthening of people's awareness of the harm of ultraviolet rays, more and more people begin to use sunscreen cosmetics to prevent the harm of ultra...
Examples
Embodiment 1
[0041] Embodiment 1: a kind of sunscreen spray, by mass parts, comprises the following components:
[0042] 40 parts water;
[0043] 4 parts humectant butylene glycol;
[0044] 3 parts thickener hydroxyethylcellulose;
[0045] 2 parts of pH regulator triethanolamine;
[0046] 3 parts emollient isohexadecane;
[0047] 3 parts emulsifier glyceryl stearate citrate;
[0048] 1.5 parts preservative phenoxyethanol;
[0049] 1.5 parts Aromatic Grapefruit;
[0050] 8 parts UV blocking absorber;
[0051] Wherein, the ultraviolet blocking absorbent comprises the following preparation steps:
[0052] (1) Put 7 parts of zinc nitrate and 8 parts of cyclohexamethylenetetramine into 120 parts of deionized water, react at 80°C for 8 minutes, then add 1.5 parts of sodium citrate, keep warm for 1.5 hours, and centrifuge to obtain For precipitation, mix the precipitate with 3 parts of zinc nitrate, 3 parts of cyclohexamethylenetetramine and 1.5 parts of sodium citrate, react at 80°C for 7 ...
Embodiment 2
[0061] Embodiment 2: a kind of sunscreen spray, by mass parts, comprises the following components:
[0062] 30 parts water;
[0063] 2 parts humectant glycerin;
[0064] 2 parts thickener xanthan gum;
[0065] 1 part pH adjuster citric acid;
[0066] 1 part emollient isododecane;
[0067] 2 parts emulsifier disodium EDTA;
[0068] 1 part preservative phenoxyethanol;
[0069] 1 part fragrance lavender;
[0070] 5 parts UV blocking absorber;
[0071] Wherein, the ultraviolet blocking absorbent comprises the following preparation steps:
[0072] (1) Put 5 parts of zinc nitrate and 5 parts of cyclohexamethylenetetramine into 100 parts of deionized water, react at 70°C for 10 minutes, then add 1 part of sodium citrate, keep warm for 1 hour, and centrifuge to obtain a precipitate. Mix the precipitate with 2 parts of zinc nitrate, 2 parts of cyclohexamethylenetetramine and 1 part of sodium citrate, react at 70°C for 10 minutes, adjust the pH to 8, keep it warm for 1 hour, was...
Embodiment 3
[0081] Embodiment 3: a kind of sunscreen spray, by mass parts, comprises the following components:
[0082] 50 parts water;
[0083] 6 parts humectant sodium hyaluronate;
[0084] 4 parts thickener carbomer;
[0085] 3 parts pH regulator sodium hydroxide;
[0086] 4 parts emollient simethicone;
[0087] 5 parts emulsifier caprylic / capric triglyceride;
[0088] 2 parts preservative phenoxyethanol;
[0089] 2 parts aromatherapy lavender;
[0090] 12 parts UV blocking absorber;
[0091] Wherein, the ultraviolet blocking absorbent comprises the following preparation steps:
[0092] (1) Put 10 parts of zinc nitrate and 10 parts of cyclohexamethylenetetramine into 150 parts of deionized water, react at 90°C for 10 minutes, then add 2 parts of sodium citrate, keep warm for 2 hours, and centrifuge to obtain a precipitate. Mix the precipitate with 4 parts of zinc nitrate, 4 parts of cyclohexamethylenetetramine and 2 parts of sodium citrate, react at 90°C for 10 minutes, adjust ...