A liquid dressing, high affinity technology, applied in the fields of resisting vector-borne diseases, medical science, bandages, etc., can solve the problems of affecting the application effect of dressings and mass promotion, promoting slow healing speed of mineralization, high material cost and high selling price, Achieve the effect of reducing scarring, good biocompatibility, and promoting rapid healing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] A fast-acting high-affinity liquid dressing, the formula of the fast-acting high-affinity liquid dressing includes the following components:
[0035]
[0036] The rest is deionized water.
[0037] Composite bacteriostatic agent in described compound bacteriostatic agent is plant extraction bacteriostatic agent VEC and octenidine hydrochloride are compounded according to the ratio of 20:5.
[0038] The preparation method of calcium, silicon ion bioactive buffer described in the present embodiment is as follows:
[0039] The first step is to select bioactive glass with calcium element ≥ 12%, silicon element ≥ 20%, and phosphorus element ≥ 1.5% to make animal-friendly bioactive glass with micropores of 1-30 nanometers after surface animal affinity treatment powder;
[0040] In the second step, put the above-mentioned animal-friendly bioactive glass powder into deionized water and soak at a constant temperature of 80°C for 72hrs, control the pH value between 10.2 and...
Embodiment 2
[0048] A fast-acting high-affinity liquid dressing, the formula of the fast-acting high-affinity liquid dressing includes the following components:
[0049]
[0050] The rest is deionized water.
[0051] Composite bacteriostatic agent in described compound bacteriostatic agent is plant extraction bacteriostatic agent VAC is formulated with octenidine hydrochloride and polyhexamethylene biguanide at a ratio of 12:5:1.
[0052] The preparation method of calcium, silicon ion bioactive buffer described in the present embodiment is as follows:
[0053] The first step is to select bioactive glass with calcium element ≥ 12%, silicon element ≥ 20%, and phosphorus element ≥ 1.5% to make animal-friendly bioactive glass with micropores of 1-30 nanometers after surface animal affinity treatment powder;
[0054] In the second step, the above-mentioned animal-friendly bioactive glass is mixed with 5% potassium hydroxide aqueous solution according to the ratio of 5:1-5, and then heate...
PUM
Property | Measurement | Unit |
---|---|---|
pore size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com