A composition and pigment technology, applied in the directions of pigment slurry, pigment-containing coating, color measuring device, etc., can solve the problem of inability to precisely control, and achieve strong practical value, refined production process, high weather resistance and stability. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Weigh 2.59 grams of PR101, 10.97 grams of PO73, 19.78 grams of PY42, and 1000 grams of CSC-B base material. Mix the above raw materials, and then apply the mixed composition evenly and evenly on the coated paper under the environmental conditions of relative humidity of 50%±5% and room temperature of 23±2°C. The wet film thickness of the coating is 250 μm, and then placed in a precision oven at 50±2°C for 3 to 4 hours to constant weight, taken out, cooled to room temperature, and obtained a physical color block.
Embodiment 2
[0024] Example 2: Weigh 2.29 grams of PR101, 10.0 grams of PO73, 19.78 grams of PY42, and 1000 grams of CSC-B base material. Manufacturing process is with embodiment 1.
Embodiment 3
[0025] Embodiment 3: Weigh 2.89 grams of PR101, 12.0 grams of PO73, 18.78 grams of PY42, and 1005 grams of CSC-B base material. Manufacturing process is with embodiment 1.
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
minimum film forming temperature | aaaaa | aaaaa |
glass transition temperature | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap