Method of using additive containing lignin to prepare cottonwood plank stuff
A technology for the preparation of additives and poplar wood, which is applied in the direction of wood compression, wood impregnation, wood impregnation, etc., can solve the problems of containing and harmful, and achieve the effects of simple production process, improved dimensional stability, and good dimensional stability.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0008] The method for preparing poplar boards by utilizing lignin-containing additives, the preparation steps are:
[0009] a. Raw material preparation: select poplar slabs, and prepare mixed solutions of two formulas, formula one: a mixed solution of lignin solution and formaldehyde solution, and formula two: a mixed solution of lignin solution and furfural solution;
[0010] B. slab impregnation treatment: the prepared poplar slabs are respectively immersed in a sealed tank filled with two kinds of mixed impregnating solutions for vacuum treatment;
[0011] c. Slab pressing: put the poplar slab after the impregnation treatment in the previous step into a hot press and heat press to obtain a poplar board.
[0012] The air-dried moisture content of poplar slab is 9%. Step a prepares the mixed solution of two kinds of formulations. Among them, formula one is: a mixed solution of lignin solution and formaldehyde solution, wherein the mixed solution is composed of: the mass per...
Embodiment 2
[0014] The method for preparing poplar boards by utilizing lignin-containing additives, the preparation steps are:
[0015] c. Raw material preparation: select poplar slabs and prepare mixed solutions of two formulas, formula one: a mixed solution of lignin solution and formaldehyde solution, and formula two: a mixed solution of lignin solution and furfural solution;
[0016] D. slab impregnation treatment: the prepared poplar slabs are respectively immersed in a sealed tank filled with two kinds of mixed impregnating solutions for vacuum treatment;
[0017] c. Slab pressing: put the poplar slab after the impregnation treatment in the previous step into a hot press and heat press to obtain a poplar board.
[0018] The air-dried moisture content of the poplar slab is 10%. Step a prepares the mixed solution of two kinds of formulations. Among them, formula one is: a mixed solution of lignin solution and formaldehyde solution, wherein the composition of the mixed solution is: t...
Embodiment 3
[0020] The method for preparing poplar boards by utilizing lignin-containing additives, the preparation steps are:
[0021] e. Raw material preparation: select poplar slabs, and prepare mixed solutions of two formulas, formula one: a mixed solution of lignin solution and formaldehyde solution, and formula two: a mixed solution of lignin solution and furfural solution;
[0022] F. slab impregnation treatment: the prepared poplar slabs are respectively immersed in a sealed tank filled with two kinds of mixed impregnating solutions for vacuum treatment;
[0023] c. Slab pressing: put the poplar slab after the impregnation treatment in the previous step into a hot press and heat press to obtain a poplar board.
[0024] The air-dried moisture content of the poplar slab is 12%. Step a prepares the mixed solution of two kinds of formulations. Among them, formula one is: a mixed solution of lignin solution and formaldehyde solution, wherein the composition of the mixed solution is: ...