Technical field
[0001] The invention relates to an environment-friendly and coal-saving agent for cement vertical kiln production. Background technique
[0002] Chinese invention patent publication CN1493542 provides an energy-saving additive for shaft kiln cement calcination, including: CaF 2 、H 2 O, Mg 6 [Si 4 o 10 ](OH) 8 , Y 2 o 3 , CeO 3 , active silicon and organosilicon, which are actually used in physical mineral products and their mass percentages are: fluorspar (fluorite) 20-35%, perlite and vermiculite 10-20%, rare earth 5-10%, serpentine Stone 15-30%, diatomaceous earth 10-20%. The shortcomings are: 1. Add fluorite and other materials, fluorite mainly contains C a f 2 , HF will be produced after the combustion reaction, and will destroy the atmospheric ozone layer when diffused into the air; 2. The proportion of cement raw materials is 0.5-0.8%, and the dosage is large. Chinese invention patent publication CN1995298 discloses a special coal-saving syn...
Examples
Embodiment 1
[0014] The cement shaft kiln environmental protection and coal-saving agent comprises the following raw materials in parts by weight:
[0015] 3 parts of coal combustion low-temperature modifier; 3 parts of composite sulfur-fixing agent; 3 parts of leavening agent;
[0016] 83 parts of combustion balance agent (including 0.83 parts of combustion inducer); 8 parts of high-efficiency sulfur-fixing agent.
[0017] The coal combustion low-temperature modifier is composed of potassium permanganate, potassium chlorate, potassium perchlorate, sodium chlorate, sodium nitrate and potassium nitrate mixed in the same proportion. The composite sulfur fixing agent is composed of sodium carbonate and calcium oxide in the same proportion. Bulking agent is paper mill waste liquid containing Na and Ca sulfonates. The combustion balance agent is a chemical waste reduction product containing about 70% sodium chloride, and the reduction product contains about 1% ammonium perchlorate. The combu...
Embodiment 2
[0020] The cement shaft kiln environmental protection and coal-saving agent comprises the following raw materials in parts by weight:
[0021] 7 parts of coal combustion low-temperature modifier; 6 parts of composite sulfur-fixing agent; 7 parts of leavening agent;
[0022] 66 parts of combustion balance agent (including 0.66 parts of combustion inducer); 14 parts of high-efficiency sulfur-fixing agent.
[0023] The coal combustion low-temperature modifier is composed of 5% potassium permanganate, 55% potassium chlorate, 15% potassium perchlorate, 15% sodium chlorate and 10% sodium nitrate. Said composite sulfur-fixing agent is sodium carbonate. Said bulking agent is paper mill waste liquid containing Na and Ca sulfonates. Said combustion balance agent is chemical waste reducing product containing 90% sodium chloride, and combustion inducer is ammonium perchlorate, which promotes rapid and complete reaction of coal. Said sulfur-fixing agent contains Fe(OH) 3 leftover iron ...
Embodiment 3
[0026] The cement shaft kiln environmental protection and coal-saving agent comprises the following raw materials in parts by weight:
[0027] 5 parts of coal combustion low-temperature modifier; 4 parts of composite sulfur-fixing agent; 5 parts of leavening agent;
[0028] 76 parts of combustion balance agent (including 0.76 parts of combustion inducer); 10 parts of high-efficiency sulfur-fixing agent.
[0029] The low-temperature modifier for coal combustion is composed of 8% potassium permanganate, 50% potassium chlorate, 12% potassium perchlorate, 15% sodium chlorate, 10% sodium nitrate and 5% potassium nitrate. Said composite sulfur-fixing agent is composed of 10% sodium carbonate, 80% calcium oxide and 10% potassium carbonate. Said bulking agent is paper mill waste liquid containing Na and Ca sulfonates. Said combustion balancing agent is chemical waste reducing product containing 80% sodium chloride, and the combustion inducer is the above-mentioned ammonium perchlora...