Groove-carving die of ceramic shell and method for processing leadless ceramic shell by using groove-carving die
A ceramic shell and processing method technology, applied to ceramic molding machines, manufacturing tools, etc., can solve problems such as scratches on the metallized layer, inconvenient operation, and hidden dangers left by the quality of the coating, so as to avoid damage, improve reliability, and improve Yield Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] (1) Install the punch in the mold for grooving on the pneumatic punching machine for use; at the same time, place the raw porcelain blank to be processed on a constant temperature heater at a temperature of 70°C to 80°C to soften for 2.5 minutes;
[0027] (2) The thickness of the green porcelain piece to be grooved is 2 mm; place the softened green porcelain piece blank on the flat mold of the groove-cutting mold, and then place the punch on the green porcelain piece, and fix the flat plate Die and punch, start the punching machine, apply 0.6 MPa pressure to the punch and flat die, and then the groove that is consistent with the knife edge on the punch can be carved on the green porcelain piece. Grooves are first made on the front side of the raw porcelain blanks; then the same method is used to carve grooves on the reverse side of the raw porcelain blanks. The depth of the groove on the front and back of the green porcelain blank is consistent with the depth of the pun...
Embodiment 2
[0033] (1) Install the punch in the mold for grooving on the pneumatic punching machine for use; at the same time, place the raw porcelain blank to be processed on a constant temperature heater at a temperature of 70°C to 80°C to soften for 5 minutes;
[0034] (2) The thickness of the green porcelain piece to be grooved is 4mm; put the softened green porcelain piece blank on the flat plate mold of the groove-cutting mold, and then put the punch on the green porcelain piece, and fix the flat plate Die and punch, start the punching machine, apply 0.6 MPa pressure to the punch and flat die, and then the groove that is consistent with the knife edge on the punch can be carved on the green porcelain piece. Grooves are first made on the front side of the raw porcelain blanks; then the same method is used to carve grooves on the reverse side of the raw porcelain blanks. The depth of the groove on the front and back of the green porcelain blank is consistent with the depth of the punc...
Embodiment 3
[0040] (1) Install the punch in the mold for grooving on the pneumatic punching machine for use; at the same time, place the raw porcelain blank to be processed on a constant temperature heater at a temperature of 70°C to 80°C to soften for 8 minutes;
[0041] (2) The thickness of the green porcelain piece to be grooved is 7mm; put the softened green porcelain piece blank on the flat mold of the groove-cutting mold, and then put the punch on the green porcelain piece, and fix the flat plate Die and punch, start the punching machine, apply 0.75MPa pressure to the punch and flat die, you can carve a groove on the raw porcelain piece that is consistent with the knife edge on the punch. Grooves are first made on the front side of the raw porcelain blanks; then the same method is used to carve grooves on the reverse side of the raw porcelain blanks. The depth of the groove on the front and back of the green porcelain blank is consistent with the depth of the punch edge, that is, th...