Superfine fiber synthetic leather, preparation method thereof and printing material composition

A technology of ultra-fine fiber and synthetic leather, which is applied in fiber treatment, textiles, papermaking, ink, etc. It can solve the problems that micro-fiber leather is not easy to wash, and achieve the effect of delicate hand feeling, full grain and excellent comprehensive physical properties

Active Publication Date: 2012-10-10
HUAFON MICROFIBER SHANGHAI
View PDF0 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] Washed synthetic leather has appeared in the field of synthetic leather, and its preparation method is generally to print and change the color of the synthetic leather that has been made, so that the synthetic leather can be washed to make the leather have a two-color effect, but so far there has been no water-washed superfine fiber synthetic leather. Because ordinary leather does not have ultra-fine fibers of 0.01 to 0.001 denier like micro-fiber leather and has a structure similar to genuine leather, the shrinkage rate, surface color adsorption and uniformity of the two washed leathers are different, and micro-fiber leather is not easy. Washing, special adjustment of printing materials and washing process is required

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Superfine fiber synthetic leather, preparation method thereof and printing material composition
  • Superfine fiber synthetic leather, preparation method thereof and printing material composition
  • Superfine fiber synthetic leather, preparation method thereof and printing material composition

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0029] Using microfiber base cloth. DE-14 is used for dry laminating release paper, the surface layer resin and solvent are according to the mass ratio 8090: DMF: MEK: TOL = 100 parts: 30 parts: 15 parts: 25 parts, add 0.1 part of dispersing aid (9565), 12 parts of toner (SP-1698: SP-4684: SP-2606=1:0.5:10..5); middle layer resin and solvent according to 8033 (dry surface layer resin): 7853N (add softener resin): MEK : DMF: TOL = 60: 40: 15: 30: 25, 20 parts of toner (White SP-2606: Black SP-1698: Red SP-4684: Yellow 2A005 = 15 parts: 0.1 parts: 4 parts: 0.9 parts ), the base material uses 5025 stock solution. Scraper distance is used respectively, the first coat is 250 μm, and the second coat is 180 μm. The temperature of the coating table is 80°C, 120°C, and 130°C for the first coat, 80°C, 120°C, and 130°C for the second coat, and 110°C, 120°C, and 135°C for the third coat. ℃, vehicle speed 5.7m / min. Superfine fiber synthetic leather can be obtained after dry veneering. ...

Embodiment 2

[0031] The microfiber base fabric is overflow dyed. DE-14 is used for dry laminating release paper, surface layer resin and solvent according to 8090: DMF: MEK: TOL = 100 parts: 30 parts: 15 parts: 25 parts, add 0.1 part of dispersing aid (9565), toner 10 parts (White SP-2606: Black SP-1698: Red SP-4684: Yellow 2A005 = 5 parts: 2 parts: 2 parts: 1 part); middle layer resin and solvent according to 8033: 7853N: MEK: DMF: TOL = 60 parts: 40 parts: 15 parts: 30 parts: 25 parts, 12 parts of toner (SP-1698: SP-4684: SP-2606 = 1: 0.5: 10..5), 5025 stock solution for primer. Scraper distance is used respectively, the first coat is 250 μm, and the second coat is 180 μm. The temperature of the coating table is 80°C, 120°C, and 130°C for the first coat, 80°C, 120°C, and 130°C for the second coat, and 110°C, 120°C, and 135°C for the third coat. , the vehicle speed is 5.7m / min. Superfine fiber synthetic leather can be obtained after dry veneering. Then carry out printing process: the r...

Embodiment 3

[0033] The microfiber base fabric is overflow dyed. DE-14 is used for dry laminating release paper, surface layer resin and solvent according to 8090: DMF: MEK: TOL = 100 parts: 30 parts: 15 parts: 25 parts, add 5 parts of dispersing aid (9565), toner 10 parts; middle layer resin and solvent according to 8033: 7853N: MEK: DMF: TOL = 60 parts: 40 parts: 25 parts: 50 parts: 25 parts, 20 parts of toner (SP-2606: 2A005: SP-1698 = 15: 4.5:0.5), the base material uses 5025 stock solution. Scraper is used for the knife distance, the first coat is 100 μm, and the second coat is 200 μm. The temperature of the coating table is 60°C, 120°C, 130°C for the first coat, 80°C, 120°C, and 130°C for the second coat, and 110°C, 120°C, and 150°C for the third coat. , speed 7m / min. Superfine fiber synthetic leather can be obtained after dry veneering. Then carry out printing process: the ratio of printing material water-based polyurethane resin and water is according to 170A: 170B: water=90: 10...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a preparation method for superfine fiber synthetic leather, which comprises the following step of: performing printing treatment, water washing, and dry rubbing on the superfine fiber synthetic leather obtained by cover making of a dry-process overlaying process, wherein a printing material in printing treatment comprises the following components in part by weight: 100 parts of waterborne polyurethane resin, 10 to 50 parts of water, preferably 20 to 40 parts of water, and 5 to 40 parts of water-based ink, preferably 10 to 30 parts of water-based ink; the temperature ofwater washing is 40 to 90DEG C, preferably 50 to 70DEG C; and the time of water washing is 15 to 50 minutes, preferably 25 to 40 minutes. The invention also discloses the superfine fiber synthetic leather prepared by the method. The superfine fiber synthetic leather is washable superfine fiber synthetic leather, and has excellent comprehensive physical properties, dual-color effect and the handfeel of natural leather. The invention also discloses a printing material composition.

Description

technical field [0001] The invention specifically relates to a superfine fiber synthetic leather, its preparation method and a printing material composition. Background technique [0002] Microfiber synthetic leather is the future development direction of synthetic leather, and has been gradually recognized by the market. Traditional polyurethane synthetic leather is generally made of raised woven or knitted fabrics. Although the appearance and feel are good, it is difficult to meet the requirements of high-end sports and leisure shoes in terms of physical properties. Synthetic leather has poor hand feeling, relatively poor physical properties, and heavy quality, which does not meet the requirements of future consumption. Microfiber synthetic leather is a new generation of artificial leather and synthetic leather products. It uses a three-dimensional network structure of non-woven fabric as the substrate, and has a polyurethane mesh and nylon bundle structure with open pore...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): D06M15/564D06N3/14C09D11/10C09D11/102
Inventor 刘勇胜刘立强王力国吴勇孙坚
Owner HUAFON MICROFIBER SHANGHAI
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products