Highly weather resistant elastic handfeel paint
A technology of high weather resistance and elastic paint, which is applied in the field of paint making, can solve the problems of poor weather resistance of hand feel elastic paint, and achieve the effect of good elasticity, good hand feeling and excellent hand feeling
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1~ Embodiment 5
[0040] The formula proportioning of the elastic paint of table 1 embodiment 6~embodiment 10
[0041]
[0042] The preparation method of above-mentioned high weather resistance type feel elastic paint is:
[0043] (1) Stir the polyaspartic acid ester modified resin, the wetting dispersant and half of the mixed solution evenly;
[0044] (2) Add polytetrafluoroethylene wax powder and stir evenly at 1200-1500 rpm;
[0045] (3) Under the condition of 300-600 r / min, slowly add matting powder, elastic powder, hand feeling additives, nano pigments, rheological additives while stirring;
[0046] (4) Stir evenly under the rotating speed condition of 1200~1500 rpm;
[0047] (5) Add drier, leveling agent and the remaining mixed solvent, and stir evenly at 300-500 rpm.
[0048] Performance Testing
[0049] In order to compare the performance of the paints provided by the present invention, the following comparative examples were adopted.
Embodiment 6~ Embodiment 10
[0059] As an improved formula, add 2 to 4% of pure polyester resin, 0.5 to 2% of hardening and wear-resistant additives, and 2 to 5% of wax paste for modification.
[0060] Polyester resin (F1190 Feiyang Chemical)
[0061] Hardening and wear-resistant additives (450 Lubrizol)
[0062] Feel wax paste (LiquiMatt6000C Lubrizol)
[0063] The ratio of each component is shown in the table below.
[0064] The formula composition of the elastic paint of table 3 embodiment 6~embodiment 10
[0065]
[0066] The preparation method of the improved formula is:
[0067] (1) Mix polyaspartate modified resin, polyester resin, wetting and dispersing agent and half of the mixed solvent, and stir for 5 minutes at 500-600 rpm;
[0068] (2) Slowly add polytetrafluoroethylene wax powder while stirring, and stir for 10 minutes at 1200-1500 rpm;
[0069] (3) Slowly add matting powder, feel wax paste, elastic powder, hardening and wear-resistant additives and nano-powder pigments while stirrin...