A kind of bleaching method of tulip tree wood for furniture
A technology of tulip tree and wood, applied in the field of wood bleaching, can solve the problem that it is difficult to meet the whiteness requirements of users
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] The bleaching method of this embodiment comprises two steps: the bleaching of low-concentration hydrogen peroxide as the main agent, and the bleaching of peracetic acid as the main agent. The first step of the main bleaching process is to prepare a bleaching solution with hydrogen peroxide, a bleach stabilizer, an activating assistant, and water. The weight ratio of each component in a 1000ml solution is: hydrogen peroxide 50g, sodium silicate 8g, sodium hydroxide 4g, and the balance being water. Immerse the wood of Liriodendron tulipifera to be bleached into the bleaching solution, raise the temperature to 70°C, and treat it for 90 minutes. Take it out, wash it with clean water, and air-dry it to the equilibrium moisture content. Use a colorimeter for color measurement, and according to the use requirements of chromaticity (whiteness, color difference), the materials are divided into two categories: those that meet the use requirements and those that fail to meet the u...
Embodiment 2
[0032] The first step of the main bleaching process is to prepare a bleaching solution with low-concentration hydrogen peroxide, bleach stabilizer, activating auxiliary agent and water. The weight ratio of each component in 1000ml solution is: hydrogen peroxide 70g, sulfuric acid Magnesium 3g, sodium hydroxide 8g, balance is water. Immerse the wood of Liriodendron chinensis to be bleached in the bleaching solution, raise the temperature to 80°C, and treat it for 60 minutes. Take it out, wash it with clean water, and air-dry it to the equilibrium moisture content. Use a colorimeter to measure the color, and according to the use requirements of the color, the materials are divided into two categories: those that meet the requirements and those that do not meet the requirements. Continue to process the materials that do not meet the requirements, and adopt the second step method. The second step bleaching solution is a mixture of glacial acetic acid, hydrogen peroxide, concentra...
Embodiment 3
[0034] In the bleaching method of this embodiment, the sample is soaked in 0.3% aqueous sodium hydroxide solution for 24 hours and then taken out. After cleaning with clear water, the sample is treated with ultrasonic waves. The medium is water, the frequency is 30 kHz, the temperature is 40 ° C, and the time 30min. The first step of the main bleaching treatment is to prepare a bleaching solution with hydrogen peroxide, bleach stabilizer, activating auxiliary agent and water. The weight ratio of each component in 1000ml solution is: 60g hydrogen peroxide, sodium silicate 6g, sodium carbonate 10g, and the balance is water. Immerse the wood of Liriodendron tulipifera to be bleached into the bleaching solution, raise the temperature to 75°C, and treat it for 80 minutes. Take it out, wash it with clean water, and air-dry it to the equilibrium moisture content. Use a colorimeter to measure the color, and according to the use requirements of the color, the materials are divided int...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com