A kind of sewing machine presser foot and preparation method thereof
A presser foot and sewing machine technology, applied in the direction of sewing machine components, presser mechanism, sewing equipment, etc., can solve the problems of high surface quality of presser foot, poor processing quality guarantee, no competitiveness, etc., and achieve easy mechanization and Automation, weakening adverse effects, and realizing the effects of mechanization and automation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] According to the components and mass percentages of Example 1 in Table 1, add aluminum, zinc, and copper into the electric furnace and heat it to 360°C to melt it. After it is completely melted, press magnesium into it with a bell jar. After the magnesium is completely melted, stir the alloy solution. , After standing still for 10min, carry out slag removal. Afterwards, the molten metal is stamped and die-casted under the condition of a pressure of 90 MPa to obtain the pressing plate and pressing rod of the sewing machine presser foot, and then the pressing plate and pressing rod are subjected to finishing machining, vibration grinding, and a layer of thickness is electroplated on the surface of the pressing plate and pressing rod Metal Ni of 15 μm. Finally, the processed press plate and press bar are assembled into the final product sewing machine presser cloth foot.
Embodiment 2
[0036] According to the components and mass percentages of Example 2 in Table 1, add aluminum, zinc, and copper into the electric furnace and heat it to 380°C to melt it. After it is completely melted, press magnesium into it with a bell jar. After the magnesium is completely melted, stir the alloy solution. , carry out slag removal after standing for 5min. Afterwards, the metal liquid is stamped and die-casted under the condition of a pressure of 85MPa to obtain the pressing plate and pressing bar of the sewing machine presser foot, and then the pressing plate and pressing bar are subjected to finishing, vibration grinding, and a layer of thickness is plated on the surface of the pressing plate and pressing bar. Metal Ni of 20 μm. Finally, the processed press plate and press bar are assembled into the final product sewing machine presser cloth foot.
Embodiment 3
[0038] According to the components and mass percentages of Example 3 in Table 1, add aluminum, zinc, and copper into the electric furnace and heat it to 400°C to melt it. After it is completely melted, press magnesium into it with a bell jar. After the magnesium is completely melted, stir the alloy solution. , After standing still for 8 minutes, carry out slag removal. Afterwards, the molten metal is stamped and die-casted under the condition of a pressure of 88 MPa to obtain the pressing plate and pressing bar of the sewing machine presser foot, and then the pressing plate and pressing bar are subjected to finishing machining, vibration grinding, and a layer of thickness is electroplated on the surface of the pressing plate and pressing bar. Metal Ni of 18 μm. Finally, the processed press plate and press bar are assembled into the final product sewing machine presser cloth foot.
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com