A fluid loss reducing agent, drilling fluid technology, applied in chemical instruments and methods, drilling compositions and other directions, can solve the problems of poor fluid loss reducing ability, poor temperature resistance and salt resistance, complex synthesis methods, etc. The effect of low, strong filtration loss reduction ability and simple synthesis method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] Take 32 parts of water according to the weight ratio and add it to the kneader (Nantong Fanshi Machinery Co., Ltd. SYH1500 kneader), add 4.5 parts of cotton cellulose, 2.0 parts of AMPS and 1.0 part of NNDMA under stirring, and stir at room temperature for 20 minutes until uniform . Stop stirring, add 0.001 parts of 10% FeCl successively 2 aqueous solution and 0.0002 parts of tert-butyl hydroperoxide to initiate the reaction. After the above raw materials were reacted for 3 hours, a cellulose graft copolymer gel was obtained. Take the gel out of the kneader, granulate it with a jelly crushing granulator, add 0.75 parts of 20% NaOH aqueous solution to hydrolyze and neutralize for 1.5 hours to obtain graft copolymer particles, and dry it at 110°C for 6 hours Pulverize, promptly make the fluid loss control agent for drilling fluid of this embodiment.
Embodiment 2
[0027] Get 35 parts of water by weight and join in the kneader (Nantong Fanshi Machinery Co., Ltd. SYH1500 type kneader), add 5.0 parts of wood pulp cellulose, 2.5 parts of AMPS and 1.5 parts of NNDMA under stirring, stir after 20 minutes at normal temperature to uniform. Stop stirring, add 0.001 parts of 10% FeCl successively 2 aqueous solution and 0.00025 parts of tert-butyl hydroperoxide to initiate the reaction. After reacting the above raw materials for 3.5 hours, a cellulose graft copolymer gel was obtained. The gel was taken out from the kneader, granulated with a jelly crushing granulator, and then 1.6 parts of 15% NaOH aqueous solution was added for hydrolysis and neutralization for 2 hours to obtain graft copolymer particles, which were dried at 115°C for 6.5 hours Pulverize, promptly make the fluid loss control agent for drilling fluid of this embodiment.
Embodiment 3
[0029] Take 36 parts of water according to the weight ratio and add it to the kneader (Nantong Fanshi Machinery Co., Ltd. SYH1500 kneader), add 6.0 parts of cotton cellulose, 3.0 parts of AMPS and 1.5 parts of NNDMA under stirring, and stir at room temperature for 20 minutes until uniform . Stop stirring, add 0.002 parts of 10% FeCl successively 2 aqueous solution and 0.0002 parts of tert-butyl hydroperoxide to initiate the reaction. After the above raw materials were reacted for 4 hours, a cellulose graft copolymer gel was obtained. The gel is taken out from the kneader, granulated with a jelly crushing granulator, and then added with 1.8 parts of 20% NaOH aqueous solution for hydrolysis and neutralization for 1 hour to obtain graft copolymer particles, which are then dried at 120°C for 5.5 hours Pulverize, promptly make the fluid loss control agent for drilling fluid of this embodiment.
PUM
| Property | Measurement | Unit |
|---|---|---|
| diameter | aaaaa | aaaaa |
| density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com