A technology of dodecanedioic acid and dodecanedioic acid crude product is applied in the purification field of dodecanedioic acid, which can solve the problem of reducing the yield of dodecanedioic acid, volatile acetic acid and methanol, increasing the load of purification, etc. problems, to achieve the effect of being conducive to environmental protection, improving purity, and reducing the generation of salt
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0064] A kind of refining method of improving dodecanedioic acid purity and yield of the present invention comprises the following steps:
[0065] ①.. Adsorption decolorization
[0066] In the dissolution reactor, put 1000 parts by weight of deionized water, add 180 parts by weight of crude dodecanedioic acid in dry weight under stirring, add 110 parts by weight of sodium hydroxide aqueous solution with a mass concentration of 30.3%, and heat up to 100 °C , the pH value is controlled between 6.0, after the material is completely dissolved, add 3 parts by weight of coconut shell-type activated carbon, and keep warm for 20 minutes for decolorization;
[0067] ②..oxidative decolorization
[0068] Filter the material treated in step ① while it is hot, rinse the filter cake with hot water at 90°C, put the filtrate and flushing liquid into the oxidation decolorization reaction kettle, raise the temperature to 98°C, and control it at 5~ Within 10 minutes, add hydrogen peroxide with...
Embodiment 2
[0079] A kind of refining method of improving dodecanedioic acid purity and yield of the present invention comprises the following steps:
[0080] ①.. Adsorption decolorization
[0081] In the dissolution reactor, put 1000 parts by weight of deionized water, add 180 parts by weight of crude dodecanedioic acid in dry weight under stirring, add 110 parts by weight of sodium hydroxide aqueous solution with a mass concentration of 30.3%, and heat up to 101 ° C , the pH value is controlled between 6.1, after the material is completely dissolved, add 4 parts by weight of coconut shell-type activated carbon, and keep warm for 30 minutes for decolorization;
[0082] ②..oxidative decolorization
[0083] Filter the material treated in step ① while it is hot, rinse the filter cake with hot water at 85°C, put the filtrate and flushing liquid into the oxidation decolorization reaction kettle, raise the temperature to 99°C, and control it at 5~ Within 10 minutes, add hydrogen peroxide wit...
Embodiment 3
[0094] A kind of refining method of improving dodecanedioic acid purity and yield of the present invention comprises the following steps:
[0095] ①.. Adsorption decolorization
[0096] In the dissolution reactor, put 1000 parts by weight of deionized water, add 180 parts by weight of crude dodecanedioic acid in dry weight under stirring, add 110 parts by weight of sodium hydroxide aqueous solution with a mass concentration of 30.3%, and heat up to 102 ° C , the pH value is controlled between 6.2, after the material is completely dissolved, add 5 parts by weight of coconut shell-type activated carbon, and keep warm for 25 minutes for decolorization;
[0097] ②..oxidative decolorization
[0098] Filter the material treated in step ① while it is hot, rinse the filter cake with hot water at 88°C, put the filtrate and flushing liquid into the oxidation decolorization reaction kettle, raise the temperature to 100°C, and control the temperature at 5~ Within 10 minutes, add hydroge...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com