A kind of warnemulin hydrochloride sustained-release granule and its preparation method and application
A technology of vornimulin hydrochloride and sustained-release granules, which can be used in pharmaceutical formulations, active ingredients of esters, bulk delivery, etc., can solve the problems of cumbersome clinical application of injection formulations, difficult to mix evenly with feed, and gastric mucosal irritation. , to solve the problem of drug palatability, prolong the maintenance time of effective blood drug concentration, and achieve the effect of stable blood drug concentration
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Publication Date
- 2019-01-25
Smart Images

Figure 1 
Figure 2 
Figure 3
Abstract
Description
technical field
[0001] The invention belongs to the technical field of animal medicines. More specifically, it relates to a warnemulin hydrochloride sustained-release granule and its preparation method and application. Background technique
[0002] Valnemulin (VLM) is a second-generation pleuromutilin-specific antibiotic for animals. It is a homologue with tiamulin and belongs to the bimectin group. It plays an antibacterial role by inhibiting protein synthesis and has a broad antibacterial spectrum. It has strong antibacterial activity, and has good antibacterial activity against different types of Mycoplasma, Mycoplasma, Streptococcus, Staphylococcus aureus, Actinobacillus, Pasteurella, Treponema hyodysenteriae and Treponema colonic piliformis, etc. With a short withdrawal period and high safety, it is the first veterinary drug premix approved by Europe and listed as a veterinary prescription drug. It has great effects in the prevention and treatment of chicken chronic re...
Examples
Embodiment 1
[0043] Example 1 Preparation of Warnemulin Hydrochloride Sustained Release Granules
[0044] The preparation steps are as follows:
[0045] S1. Weigh each carrier auxiliary material according to the following formula ratio (based on the total mass as 100g):
[0046] Warnemulin Hydrochloride 20%;
[0047] Stearyl Alcohol 75%;
[0048] Beeswax 5%;
[0049] Heat to melt at 80°C and mix well;
[0050] S2. adding warnemulin hydrochloride to the carrier auxiliary material obtained in S1, and stirring evenly to obtain a mixed material;
[0051] S3. Cool the mixed material obtained in S2 to 60-80°C, and perform the stage of fluidized bed spray granulation and spheroidization, the temperature of the fluidized air in the granulation and spheroidization stage is 25°C; the fluidized bed spray droplets The line speed is 10-160 m / s;
[0052]S4. Cool, sieve, and collect to obtain 20% warnemulin hydrochloride sustained-release granules.
Embodiment 2
[0053] Example 2 Preparation of Warnemulin Hydrochloride Sustained Release Granules
[0054] The preparation steps are as follows:
[0055] S1. Weigh each carrier auxiliary material according to the following formula ratio (based on the total mass as 100g):
[0056] Warnemulin Hydrochloride 10%;
[0057] Glyceryl Monostearate 80%;
[0058] Beeswax 10%;
[0059] Heat to melt at 70°C and mix well;
[0060] S2. adding warnemulin hydrochloride to the carrier auxiliary material obtained in S1, and stirring evenly to obtain a mixed material;
[0061] S3. Cool the mixed material obtained in S2 to 60-80°C, and carry out the stage of fluidized bed spray granulation and spheroidization, the temperature of the fluidized air in the granulation and spheroidization stage is 20°C; The line speed is 40-80 m / s;
[0062] S4. Cool, sieve, and collect to obtain 10% warnemulin hydrochloride sustained-release granule preparation.
Embodiment 3
[0063] Example 3 Preparation of Warnemulin Hydrochloride Sustained Release Granules
[0064] The preparation steps are as follows:
[0065] S1. Weigh each carrier auxiliary material according to the following formula ratio (based on the total mass as 100g):
[0066] Warnemulin Hydrochloride 25%;
[0067] Animal fat 70%;
[0068] Carnauba Wax 5%;
[0069] Heat to melt at 95°C and mix well;
[0070] S2. adding warnemulin hydrochloride to the carrier auxiliary material obtained in S1, and stirring evenly to obtain a mixed material;
[0071] S3. Cool the mixed material obtained in S2 to 60-80°C, and carry out the stage of fluidized bed spray granulation and spheroidization, the fluidized air temperature in the granulation and spheroidization stage is 30°C; the fluidized bed spray droplets The line speed is 40-80 m / s;
[0072] S4. Cool, sieve, and collect to obtain 25% warnemulin hydrochloride sustained-release granule preparation.