A production method and fusible interlining technology, applied in the dyeing method, textile decoration, textile material treatment, etc., can solve the problems of degradation loss, dull surface, poor color fastness, etc., and achieve convenient operation and coating surface The effect of brightness and excellent product performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] The interlining fabric has a width of 48.5 inches and a yarn count of 60 s ×60 s , The density is 68×52 pieces / inch;
[0025] A method for producing pure cotton napped colored bright fusible interlining, comprising the steps of turning, napping, scouring, bleaching, dyeing, shrink-proof finishing, bright powder dot coating, and mechanical preshrinking;
[0026] During the napping process, one side is stretched twice, the cylinder speed is 75 rpm, the clockwise roller speed is 700rpm, the cylinder pressure of the clockwise roller is 0.20Mpa, the cylinder pressure of the counterclockwise roller is 0.25Mpa, the counterclockwise roller speed is 800rpm; the tension of the upper cloth guide roller is 1.8 %, the tension of the front cloth guide roller is 2.8%, the tension of the rear cloth guide roller is 1.9%, and the cloth feeding speed is 14-16m / min. After napping, the surface of the fabric is covered with a layer of uniform fluff. After the brushed fusible interlining i...
Embodiment 2
[0036] The interlining fabric has a width of 48.5 inches and a yarn count of 80 s ×80 s , The density is 80×60 pieces / inch;
[0037] A method for producing pure cotton napped colored bright fusible interlining, comprising the steps of turning, napping, scouring, bleaching, dyeing, shrink-proof finishing, bright powder dot coating, and mechanical preshrinking;
[0038] During the napping process, one side is stretched twice, the cylinder speed is 75 rpm, the clockwise roller speed is 700rpm, the cylinder pressure of the clockwise roller is 0.20Mpa, the cylinder pressure of the counterclockwise roller is 0.25Mpa, the counterclockwise roller speed is 800rpm; the tension of the upper cloth guide roller is 1.8 %, the tension of the front cloth guide roller is 2.8%, the tension of the rear cloth guide roller is 1.9%, and the cloth feeding speed is 14-16m / min. After napping, the surface of the fabric is covered with a layer of uniform fluff. After the brushed fusible interlining ...