Method for preparing biomass fuel with fresh cow dung as main raw material
A biomass fuel and main raw material technology, applied in biofuel, waste fuel, fuel, etc., can solve problems such as environmental pollution, high moisture content of cow dung and difficult fermentation, etc., to improve combustion efficiency, facilitate fuel molding, and carbon-nitrogen ratio Improved effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] A method for preparing biomass fuel with fresh cow dung as the main raw material, the specific steps are:
[0032] 1) Raw material pretreatment: crush the discarded mushroom sticks, dry them naturally to make the moisture content below 10wt%, and prepare the mushroom sticks; heat the discarded shells at a heating rate of 15°C / min Calcining at 900°C for 5 hours to obtain calcined shell powder;
[0033] 2) Fermentation: Mix 80wt% of fresh cow dung, 15wt% of mushroom sticks and 5wt% of calcined shell powder to make a mixture; The moisture content of the material is reduced to 25wt%; the nitrogen fixation-desulfurization composite microorganism is composed of Pseudomonas putida ( Pesudomonas putida ), Pseudomonas flavinogenes ( Cellulomonas flavigena ), Aspergillus oryzae ( Aspergillus oryzae ), Bacillus licheniformis ( Bacillus licheniformis ) and Streptomyces griseus ( Streptomyces griseus ) is compounded according to the mass ratio of 3:5:2:1:6, and the amount...
Embodiment 2
[0041] A method for preparing biomass fuel with fresh cow dung as the main raw material, the specific steps are:
[0042] 1) Raw material pretreatment: crush the discarded mushroom sticks, dry them naturally to make the moisture content below 10wt%, and prepare the mushroom sticks; heat the discarded shells at a heating rate of 30°C / min Calcining at 1100°C for 3 hours to obtain calcined shell powder;
[0043] 2) Fermentation: Mix 80wt% of fresh cow dung, 17wt% of mushroom sticks and 3wt% of calcined shell powder to make a mixture; The moisture content of the material is reduced to 20wt%; the nitrogen fixation-desulfurization composite microorganism is composed of Pseudomonas putida ( Pesudomonas putida ), Pseudomonas flavinogenes ( Cellulomonas flavigena ), Aspergillus oryzae ( Aspergillus oryzae ), Bacillus licheniformis ( Bacillus licheniformis ) and Streptomyces griseus ( Streptomyces griseus ) is compounded according to the mass ratio of 3:5:2:1:6, and the amoun...
Embodiment 3
[0051] A method for preparing biomass fuel with fresh cow dung as the main raw material, the specific steps are:
[0052] 1) Raw material pretreatment: crush the discarded mushroom sticks, dry them naturally to make the moisture content below 10wt%, and prepare mushroom sticks; heat the discarded shells at a heating rate of 20°C / min Calcining at 1000°C for 4 hours to obtain calcined shell powder;
[0053] 2) Fermentation: Mix 80wt% of fresh cow dung, 16wt% of mushroom sticks and 4wt% of calcined shell powder to make a mixture; The moisture content of the material is reduced to 25wt%; the nitrogen fixation-desulfurization composite microorganism is composed of Pseudomonas putida ( Pesudomonas putida ), Pseudomonas flavinogenes ( Cellulomonas flavigena ), Aspergillus oryzae ( Aspergillus oryzae ), Bacillus licheniformis ( Bacillus licheniformis ) and Streptomyces griseus ( Streptomyces griseus ) is compounded according to the mass ratio of 3:5:2:1:6, and the amount of...
PUM
Property | Measurement | Unit |
---|---|---|
combustion efficiency | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com