Pesticide nano emulsion in water and preparing method thereof
A water-emulsion and nano-technology, applied in the field of pesticides, can solve the problems of poor stability of water-emulsion, achieve good stability, low production cost, and facilitate absorption and utilization
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] Add 20% of Methochlor, 30% of Terbutylazine, 15% of D-Limonene, and 20% of Starch Sodium Octenyl Phosphate into a 50mL flat-bottomed glass bottle in turn, add a magnet, and stir and mix at a speed of 1500rpm for 15min; Take 3% ethylene glycol, 5% xanthan gum, 0.5% methyl polysiloxane, make up to 100% with deionized water, and mix it in another 50mL flat-bottomed glass bottle at a speed of 1500rpm for 15min; at room temperature, Under the condition of stirring at a rotating speed of 2000 rpm, the water phase was added to the oil phase, and stirred and mixed for 30 minutes to form a nano-water emulsion with a mass percentage of methoxam and terbuthylazine of 50%.
Embodiment 2
[0033] Add 50% of methoxam, 10% of terbutyzine, 10% of biodiesel, and 10% of isooctyl polyoxyethylene ether into a 50mL flat-bottomed glass bottle in turn, add magnets, stir and mix at 2000rpm for 10min; take urea 8 %, 1% hydroxypropyl cellulose, 0.3% isooctyl alcohol, deionized water to make up to 100%, in another 50mL flat-bottom glass bottle, stir and mix at 2000rpm for 10min; at room temperature, stir at 1500rpm Under certain conditions, the water phase was added to the oil phase, and stirred and mixed for 40 minutes to form a nano-water emulsion with a mass percentage of methoxam and terbuthylazine of 60%.
Embodiment 3
[0035] Add 1% of methoxam, 9% of terbutyzine, 5% of N-dodecylpyrrolidone, and 2% of polyoxyethylene stearate into a 50mL flat-bottomed glass bottle in turn, add a magnet, and stir and mix at a speed of 1000rpm 15min; Take 1% sorbitol, 1% gum arabic, make up to 100% with deionized water, put in another 50mL flat-bottomed glass bottle, stir and mix at 1000rpm for 15min; The water phase was added to the oil phase, and stirred and mixed for 30 minutes to form a nanoemulsion in water with 10% by mass of methoxam and terbuthylazine.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com