Aqueous spraying profile preparation method
A profile, water-based technology, applied in the direction of coating, latex paint, etc., can solve the problems of high volatility of organic solvents, health damage, difficult to decompose, etc., to achieve high gloss, bright surface, safe spraying and use process effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0016] A kind of preparation method of water-based spray profile, comprises the following steps:
[0017] Step 1. Carry out washing, degreasing, water washing, conversion coating, two water washings, drying, and removal of the hanging substrate in sequence;
[0018] Step 2. The profiles processed in step 1 are put on the shelves, sprayed with water-based paint, cured, and removed from the shelves in sequence, and finally packaged as finished water-based sprayed profiles;
[0019] The curing temperature in the second step is 180-200°C.
[0020] Calculated according to mass percentage, the proportioning scheme of described water-based paint is as follows:
[0021] Resin paint: 25-30%, alcohol solvent 25-45%, water 25-45%; the sum of the percentages of the above components is 100%.
Embodiment 1
[0023] A kind of preparation method of water-based spray profile, comprises the following steps:
[0024] Step 1. Carry out washing, degreasing, water washing, conversion coating, two water washings, drying, and removal of the hanging substrate in sequence;
[0025] Step 2. The profiles processed in step 1 are put on the shelves, sprayed with water-based paint, cured, and removed from the shelves in order to be packaged as finished water-based sprayed profiles;
[0026] The curing temperature in the second step is 180°C.
[0027] The proportioning scheme of each component of described water-based paint is as follows:
[0028] Resin paint: 25%, alcohol solvent 35%, water 40%.
Embodiment 2
[0030] A kind of preparation method of water-based spray profile, comprises the following steps:
[0031] Step 1. Carry out washing, degreasing, water washing, conversion coating, two water washings, drying, and removal of the hanging substrate in sequence;
[0032] Step 2. The profiles processed in step 1 are put on the shelves, sprayed with water-based paint, cured, and removed from the shelves in order to be packaged as finished water-based sprayed profiles;
[0033] The curing temperature in the second step is 190°C.
[0034] The proportioning scheme of each component of described water-based paint is as follows:
[0035] Resin paint: 30%, alcohol solvent 45%, water 25%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com