A kind of anti-insect slow-release product and preparation method thereof
A slow-release and insect-proof technology, applied in the field of daily chemical products, can solve the problems of high drug-carrying residue rate, low drug-carrying residue rate, unstable slow-release amount, etc., so as to improve the slow-release effect, reduce the residual rate, and reduce the loss. rate effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0061] The present embodiment provides a mosquito repellent sustained-release product, wherein the base material is porous polystyrene (macropore refers to a hole with a pore diameter greater than or equal to 50 nm) whose macropore volume accounts for more than 82% of the total pore volume, and the synthetic porous polystyrene The ethylene emulsion is composed of the following components in mass percentage: 15.3% styrene, 1.6% divinylbenzene, 0.5% azobisisobutyronitrile, 1.6% emulsifier, and 81.0% deionized water.
[0062] The size of the molding die is a cylindrical aluminum container with a diameter of 55mm and a thickness of 3mm. The product is made according to the process flow. The weight of the porous polystyrene is 2g, and the pyrethroid is loaded with 300mg to obtain a mosquito repellent slow-release product.
Embodiment 2
[0064] This embodiment provides a mosquito repellent sustained-release product, wherein the base material is porous polystyrene whose macropore volume accounts for more than 82% of the total pore volume, and the emulsion of the synthesized porous polystyrene consists of the following groups in mass percentage: Composition: styrene 17.5%, divinylbenzene 2.0%, azobisisobutyronitrile 0.6%, emulsifier 1.8%, deionized water 78.1%.
[0065] The size of the molding die is a cylindrical aluminum container with a diameter of 55mm and a thickness of 3mm. The product is made according to the process flow. The weight of the porous polystyrene is 2g, and the pyrethroid is loaded with 300mg to obtain a mosquito repellent slow-release product.
Embodiment 3
[0067] This embodiment provides a mosquito repellent sustained-release product, wherein the base material is porous polystyrene whose macropore volume accounts for more than 82% of the total pore volume, and the emulsion of the synthesized porous polystyrene consists of the following groups in mass percentage: Composition: styrene 10.6%, divinylbenzene 1.1%, azobisisobutyronitrile 0.5%, emulsifier 2.7%, deionized water 85.1%.
[0068] The size of the molding die is a cylindrical aluminum container with a diameter of 55mm and a thickness of 3mm. The product is made according to the process flow. The weight of the porous polystyrene is 2g, and the pyrethroid is loaded with 300mg to obtain a mosquito repellent slow-release product.
PUM