A technology for cigarette mainstream smoke and coating materials, applied in the direction of anti-corrosion coatings, coatings, etc., can solve the problems of high cost, large dosage, poor interception effect on phenol, etc., and achieve the goal of reducing phenol release and good coating performance Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] Add 15g glucose pentaacetate, 6g propylene glycol, 2g polyvinyl acetate emulsion, 1g fumed silica, 0.1g potassium sorbate, and 0.1g simethicone into 76g water, and stir for 1 hour. The obtained liquid coating material has a solid content of 22.8% and a Brookfield viscosity of 90 cps (25°C).
Embodiment 2
[0032] Add 37g of enzymatically treated glucose pentaacetate, 13g of glycerol, 5g of polyvinyl acetate emulsion, 2g of fumed silica, 0.3g of potassium sorbate, and 0.2g of simethicone into 43g of water, and stir One hour is enough. The obtained liquid coating material has a solid content of 53.5% and a Brookfield viscosity of 280 cps (25°C).
Embodiment 3
[0034] Add 30g sucrose octaacetate, 5g propylene glycol, 10g glycerol, 4g polyvinyl acetate emulsion, 4g fumed silica, 0.2g potassium sorbate, 0.2g simethicone into 47g water and stir for 1 hour That's it. The obtained liquid coating material has a solid content of 49.1% and a Brookfield viscosity of 395 cps (25°C).