[0037] Weighing: ε-polylysine 0.1g, propylene glycol 2g, sodium dodecylbenzenesulfonate 0.1g, borneol 0.5g, vitamin E 0.05g, pure water 100mL.
[0038] (1) Put sodium dodecylbenzenesulfonate and vitamin E in absolute ethanol, pour the alcohol solution into pure water and stir, remove the ethanol in the solution in a constant temperature water bath at 80°C for 6 minutes, and cool to room temperature to obtain a surfactant aqueous solution.
[0039] (2) Add ε-polylysine to the aqueous surfactant solution in (1), and stir in a constant temperature water bath at 40°C to dissolve the ε-polylysine completely.
[0040] (3) Add propylene glycol and borneol to (2), stir in a constant temperature water bath at 40°C, and stir at 200r / min for 1min.
[0041] (4) adding lactic acid to adjust the pH value of step (3) to 4.5.
[0042] (5) Sterilize the prepared solution (4).
Embodiment 2
[0044] Weighing: ε-polylysine 3g, glycerol 8g, sophorolipid 0.15g, borneol 1g, vitamin E 0.07g, pure water 100mL.
[0045] (1) Dissolve sophorolipids and vitamin E in absolute ethanol, pour the alcohol solution into pure water and stir, remove the ethanol in the solution in a constant temperature water bath at 85°C for 8 minutes, and cool to room temperature to prepare an aqueous surfactant solution.
[0046] (2) Add ε-polylysine to the aqueous surfactant solution in (1), and stir in a constant temperature water bath at 45°C to dissolve ε-polylysine completely.
[0047] (3) Add glycerol and borneol to (2), stir in a constant temperature water bath at 45°C, and stir at 300r / min for 2min.
[0048] (4) adding sodium lactate to adjust the pH value of step (3) to be 5.
[0049] (5) Sterilize the prepared solution (5).
Embodiment 3
[0051] Weighing: ε-polylysine 5g, sodium hyaluronate 15g, lecithin 0.2g, borneol 1.5g, vitamin E 0.09g, pure water 100mL.
[0052] (1) Dissolve lecithin and vitamin E in absolute ethanol, pour the alcohol solution into pure water and stir, remove the ethanol in the solution in a constant temperature water bath at 90°C for 10 minutes, and cool to room temperature to prepare an aqueous surfactant solution.
[0053](2) Add ε-polylysine to the surfactant aqueous solution in (1), and stir in a constant temperature water bath at 50°C to dissolve ε-polylysine completely.
[0054] (3) Add sodium hyaluronate and borneol to (2), stir in a constant temperature water bath at 50°C, and stir at 400r / min for 3min.
[0055] (4) adding lactic acid to adjust the pH value of step (3) to 5.5.
[0056] (5) Sterilize the prepared solution (3).
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com