Reverse osmosis prevention type liquid absorbing core
A technology of anti-reverse seepage and absorbent core, which is applied in the direction of absorbent pads, medical science, bandages, etc., and can solve problems such as reverse seepage of polymer composite cores
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0037] Embodiment 1: An anti-reverse seepage type liquid-absorbent core, comprising an absorbent layer 1 bonded by an adhesive layer 3 and an anti-reverse seepage film 2, and the anti-reverse seepage film 2 includes an outer layer 21 and an intermediate layer 22 arranged in sequence and outer layer 21. The anti-reverse seepage type liquid absorbent core is prepared by the following method:
[0038] (1) Preparation of anti-reverse osmosis membrane 2:
[0039] ① Cotton fiber pretreatment: put the cotton fiber into the pretreatment container, add ethanol solution with a purity of 85wt% ethanol, soak for 0.5hr, take out the cotton fiber, and dry it by blowing at 35°C; cotton fiber and ethanol aqueous solution The mass ratio is 1:2.5;
[0040] 2. the preparation of compound I: the cotton fiber, nano-calcium carbonate and microcrystalline cellulose through pretreatment are pulverized respectively, and cotton fiber crosses 5 mesh sieves, and nano-calcium carbonate and microcrystall...
Embodiment 2
[0048] Embodiment 2: An anti-reverse seepage type liquid-absorbent core, comprising an absorbent layer 1 bonded by an adhesive layer 3 and an anti-reverse seepage film 2, and the anti-reverse seepage film 2 includes an outer layer 21 and an intermediate layer 22 arranged in sequence and outer layer 21. The anti-reverse seepage type liquid absorbent core is prepared by the following method:
[0049] (1) Preparation of anti-reverse osmosis membrane 2:
[0050] ① Cotton fiber pretreatment: put cotton fiber into a pretreatment container, add ethanol solution with a purity of 75wt% ethanol, take out the cotton fiber after soaking for 2 hours, and blow dry it at 40°C; Mass ratio 1:3.0;
[0051] 2. the preparation of compound I: the cotton fiber, nano-calcium carbonate and microcrystalline cellulose through pretreatment are pulverized respectively, and cotton fiber crosses 5 mesh sieves, and nano-calcium carbonate and microcrystalline cellulose cross 20 mesh sieves; Put the cotton...
Embodiment 3
[0059] Embodiment 3: An anti-reverse osmosis type liquid-absorbent core, the difference from Embodiment 1 is that in the mixture I, lactose is replaced with an equal amount of cotton fiber.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 