Reverse osmosis preventing type paper diaper
A technology of anti-reverse osmosis and paper diapers, which is applied in the fields of medical science, clothing, underwear, etc., and can solve problems such as reverse osmosis
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1a
[0051] Embodiment 1a: an anti-reverse osmosis membrane 31 , comprising an outer layer 311 , an intermediate layer 312 and an outer layer 311 arranged in sequence. The anti-reverse osmosis membrane 31 is prepared by the following method:
[0052] ① Cotton fiber, commercially available cotton fiber is pre-treated with ethanol aqueous solution before use, and the specific steps are:
[0053] Put the cotton fiber into the pretreatment container, add the ethanol aqueous solution with the purity of ethanol as 85wt%, take out the cotton fiber after soaking for 0.5 hr, and dry it by blowing at 35°C; the mass ratio of cotton fiber and ethanol aqueous solution is 1:2.5;
[0054] 2. the preparation of compound I: the cotton fiber, nano-calcium carbonate and microcrystalline cellulose through pretreatment are pulverized respectively, and cotton fiber crosses 5 mesh sieves, and nano-calcium carbonate and microcrystalline cellulose cross 20 mesh sieves; Put the cotton fiber into a mixing c...
Embodiment 1b
[0061] Embodiment 1b: An anti-reverse osmosis membrane 31 , comprising an outer layer 311 , an intermediate layer 312 and an outer layer 311 arranged in sequence. The anti-reverse osmosis membrane 31 is prepared by the following method:
[0062] ① Cotton fiber, commercially available cotton fiber is pre-treated with ethanol aqueous solution before use, and the specific steps are:
[0063] Put the cotton fiber into the pretreatment container, add the ethanol solution with the purity of 75wt% ethanol, take out the cotton fiber after soaking for 2 hours, and blow dry at 40°C; the mass ratio of cotton fiber and ethanol solution is 1:3.0;
[0064] 2. the preparation of compound I: the cotton fiber, nano-calcium carbonate and microcrystalline cellulose through pretreatment are pulverized respectively, and cotton fiber crosses 5 mesh sieves, and nano-calcium carbonate and microcrystalline cellulose cross 20 mesh sieves; Put the cotton fiber into a mixing container, add the prescribe...
Embodiment 1c
[0071] Embodiment 1c: a kind of anti-reverse osmosis membrane 31, differs from embodiment 1a in that before the mixture I is mixed, the cotton fiber is not pre-treated by soaking in an aqueous ethanol solution, that is, the cotton fiber directly adopts commercially available cotton fiber.