Embodiment 1
[0022] First weigh according to the mass percentage: 30% of cementitious material, 50% of natural graded medium sand, 19.3% of stone, 0.3% of polycarboxylate superplasticizer, 0.1% of hemp fiber, 0.1% of air-entraining agent, and defoamer 0.2%, mix the above raw materials in a gravity-free mixing mixer for 8 minutes to obtain the spray dry powder; then weigh 100 parts of the above spray dry powder and 10 parts of water according to the parts by weight, and set aside.
Embodiment 2
[0024] First weigh according to the mass percentage: 34% of cementitious material, 50% of natural graded medium sand, 15.5% of stone, 0.3% of polycarboxylate superplasticizer, 0.05% of hemp fiber, 0.05% of air-entraining agent, defoamer 0.1%, mix the above raw materials in a gravity-free mixing mixer for 8 minutes to obtain the spray dry powder; then weigh 100 parts of the above spray dry powder and 11 parts of water according to the parts by weight, and set aside.
Embodiment 3
[0026] First weigh according to the mass percentage: 39% of cementitious material, 45% of natural graded medium sand, 15.4% of stone, 0.25% of polycarboxylate superplasticizer, 0.1% of hemp fiber, 0.05% of air-entraining agent, defoamer 0.2%, mix the above raw materials in a gravity-free mixing mixer for 12 minutes to obtain spray dry powder; then weigh 100 parts of the above spray dry powder and 12 parts of water according to the parts by weight, mix the spray dry powder and water, stir evenly, and transport to spraying The hardening accelerator is transported to the spray gun of the above-mentioned spraying equipment through wind pressure for uniform spraying. The spraying rate is 100L / min, and the thickness of one-time spraying is 100mm, so as to obtain the spraying material for the snowmobile and sled track. Example 4
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
compressive strength | aaaaa | aaaaa |
compressive strength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com