Tail box door spring surface spraying and flocking method
A technology of surface spraying and flocking, which is applied to the device for coating liquid on the surface, special surfaces, coatings, etc. Stable performance, stable flocking effect and excellent effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] The present invention provides a method for flocking by spraying on the surface of a trunk door spring. The method is as follows: (1) Prepare waterproof and oil-proof polyurethane flocking glue, and clean the trunk door spring to make the surface smooth.
[0019] Among them, the components of the waterproof and oil-proof polyurethane flocking glue and the weight percentage of each component are: resin base:
[0020] 45%, isocyanate: 15%, diphenylmethane diisocyanate: 13%, combined polyether: 20% and auxiliary components: 7%; the composition of the resin base and the total mass percentage of each component in the resin base are: Silicone resin: 45%, ASA resin: 40% and filler: 15%; the composition of the combined polyether and the mass percentage of each component in the total mass of the combined polyether are: polyether monomer: 66%, uniform foam Agent: 15%, cross-linking agent: 3%, catalyst: 5% and foaming agent: 11%; the composition of the auxiliary components and the...
Embodiment 2
[0024] The present invention provides a method for flocking by spraying on the surface of a trunk door spring. The method is as follows: (1) Prepare waterproof and oil-proof polyurethane flocking glue, and clean the trunk door spring to make the surface smooth.
[0025] Among them, the components of the waterproof and oil-proof polyurethane flocking glue and the weight percentage of each component are: resin base:
[0026] 62%, isocyanate: 8%, diphenylmethane diisocyanate: 5%, combined polyether: 20% and auxiliary components: 5%; the composition of the resin base and the total mass percentage of each component in the resin base are: Silicone resin: 62%, ASA resin: 28% and filler: 10%; the composition of the combined polyether and the mass percentage of each component in the total mass of the combined polyether are: polyether monomer: 80%, uniform foam Agent: 8%, cross-linking agent: 3%, catalyst: 2% and foaming agent: 7%; the composition of the auxiliary components and the tot...
Embodiment 3
[0030] The present invention provides a method for flocking by spraying on the surface of a trunk door spring. The method is as follows: (1) Prepare waterproof and oil-proof polyurethane flocking glue, and clean the trunk door spring to make the surface smooth.
[0031] Among them, the components of the waterproof and oil-proof polyurethane flocking glue and the weight percentage of each component are: resin base:
[0032] 51%, isocyanate: 9%, diphenylmethane diisocyanate: 10%, combined polyether: 24% and auxiliary components: 6%; the composition of the resin base and the total mass percentage of each component in the resin base are: Silicone resin: 53%, ASA resin: 34% and filler: 13%; the composition of the combined polyether and the mass percentage of each component in the total mass of the combined polyether are: polyether monomer: 72%, uniform foam Agent: 10%, cross-linking agent: 5%, catalyst: 4% and foaming agent: 9%; the composition of auxiliary components and the total...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com