A blended yarn and pretreatment technology, applied in liquid/gas/steam yarn/filament treatment, fiber treatment, yarn and other directions, can solve the problem of not easy to restore the circular cavity wall, increase the kapok fiber crushing wear, can not be very fast It can solve the problems of kapok fiber loss and other problems, achieve good hydrophilicity and antistatic performance, save energy consumption, and is not easy to wear and tear
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The blended yarn count that present embodiment adopts is 40 pounds;
[0026] S1. At 40-50°C, use RFS-222 fatty acid organic amine compound and add water to fully reconcile and evenly prepare a treatment solution containing 10% of the compound;
[0027] S2. Humidification treatment of impregnated blended yarn: Put the upper part of the bobbin downwards into the prepared treatment solution. The upper part is placed upwards, so that the treatment liquid flows into the lower part of the non-impregnated bobbin from top to bottom; the bobbin is formed by winding cotton and kapok blended yarn on the bobbin;
[0028] S3. Cover with a closed plastic film, cover and stew the yarn to fuse with the infiltration solution, and leave it for 6-8 hours; after 6 hours, start to test the humidity and moisture regain;
[0029] S4. Use a portable yarn moisture meter of model YG201B to test the humidity and moisture regain, the two are respectively: 55-75% and 15-22%, and then weave on the ...
Embodiment 2
[0031] The blended yarn count that present embodiment adopts is 10 pounds;
[0032] S1. At 40-50°C, use RFS-222 fatty acid organic amine compound and add water to fully reconcile and evenly prepare a treatment solution containing 10% of the compound;
[0033] S2. Humidification treatment of impregnated blended yarn: Put the upper part of the bobbin downwards into the prepared treatment solution. The upper part is placed upwards, so that the treatment liquid flows into the lower part of the non-impregnated bobbin from top to bottom; the bobbin is formed by winding cotton and kapok blended yarn on the bobbin;
[0034] S3. Cover with a closed plastic film, cover and stew the yarn to fuse with the infiltration solution, and leave it for 5-6 hours; after 5 hours, start to test the humidity and moisture regain;
[0035] S4. Use a portable yarn moisture meter of model YG201B to test the humidity and moisture regain, the two are respectively: 55-75% and 15-22%, and then weave on the ...