Oil-resistant sealing rubber ring and vulcanization method
A technology for sealing rubber rings and rubber rings, which is applied in the direction of engine sealing, mechanical equipment, engine components, etc., can solve the problem that the oil resistance performance has not been significantly improved, and achieve the effect of improving oil resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0053] The raw rubber slurry is mixed with the micro air cells to form a mixed slurry, which is injected into the mold and cured to form the rubber ring body 1, and the rubber ring body 1 is placed in the heating chamber for steam vulcanization, and the micro air cells in the rubber ring body 1 Heat and rupture from the outer layer to the inner layer in turn to form an air cavity 2. The gaseous hot sulfur content enters the air cavity 2 inside the rubber ring body 1 for vulcanization. The vulcanized rubber ring body 1 is immersed in the fluorinated rubber slurry, taken out and cured After that, an oil-resistant sealing rubber ring is formed.
[0054] The annular rubber ring body 1 is provided with honeycomb-shaped and interconnected air chambers 2, the outer surface of the rubber ring body 1 is covered with a fluorinated rubber layer 4, the rubber ring body 1 provides sufficient mechanical elasticity, and the fluorinated rubber layer 4 has sufficient oil resistance;
[0055] ...
Embodiment 2
[0057] The magnetic powder is used as a condensation nucleus, and the solid gas is condensed in a low temperature and high pressure environment to form composite powdery particles. After the particles are accelerated and bombarded with the plastic melt film, small particles wrapped by the plastic melt are formed. After the temperature rises, the solid The gas powder recovers to gaseous state and expands to form micro-airbags. However, during this process, there are some plastic films that do not completely cover the magnetic powder and enter the separation tank. The liquid with a density less than that of solid plastic is filled in the separation tank, and the objects floating on the liquid surface are micro-airbags. , place the mixed slurry in a uniform constant magnetic field, and then perform the curing operation after the micro-airbags stop moving, use the magnetic field to arrange the magnetic micro-airbags evenly and tightly, and the air cavity 2 generated after the micro-...