Production method of light soft long hair rabbit wool and mink cashmere blend fiber product
A blended fiber and production method technology, applied in the field of rabbit and mink, can solve the problems of substandard quality and spinnability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Embodiment 1: a kind of production method of soft long-haired rabbit down and mink down blended fiber product is characterized in that it also comprises the following steps: Step A: select mink down fiber with a fineness of 12 μm and a fiber length of 12 mm, and select a fineness between 12 μm and 12 mm. The long-haired rabbit down fiber with a fiber length of 14 μm and a fiber length of 40 mm is mixed into a woolen material in terms of mass percentage, of which mink down fiber accounts for 60% and long-haired rabbit down fiber accounts for 40%. Step B: Blend the blended fibers. When blending, mink down fiber is opened separately for 1-2 times, long-haired rabbit down fiber is opened separately for 1-2 times, and the two fibers are mixed and laid together for 3 times. , after adding the blending agent, beat it again; finally carry out bagging treatment; in terms of mass percentage, the blending agent includes 3% and hair oil FX-906, 1% antistatic agent FX-AS301, and 1% s...
Embodiment 2
[0018] Embodiment 2: a kind of production method of soft long-haired rabbit down and mink down blended fiber product is characterized in that it also comprises the following steps: Step A: select the mink down fiber with a fineness of 13 μm and a fiber length of 15 mm, and select a fineness in the range of 15 mm. The long-haired rabbit down fiber with a fiber length of 18 μm and between 50 mm is mixed into a woolen material in terms of mass percentage, wherein mink down fiber accounts for 80% and long-haired rabbit down fiber accounts for 20%. Step B: Blend the blended fibers. When blending, mink down fiber is opened separately for 1-2 times, long-haired rabbit down fiber is opened separately for 1-2 times, and the two fibers are mixed and laid together for 3 times. , after adding the blending agent, beat it again; finally carry out bagging treatment; in terms of mass percentage, the blending agent includes 3% and hair oil FX-906, 1% antistatic agent FX-AS301, and 1% strengthen...
Embodiment 3
[0021] Embodiment 3: a kind of soft long-haired rabbit down and mink down blended fiber product production method, it is characterized in that also comprising the following steps: in step A, select the mink down fiber with fineness at 12.5 μm, fiber length at 14mm, Select long-haired rabbit down fibers with a fineness of 15.6 μm and a fiber length of 46 mm, and mix the two into a woolen material in terms of mass percentage, of which mink down fibers account for 70% and long-haired rabbit down fibers account for 30%. Step B: Blend the blended fibers. When blending, mink down fiber is opened separately for 1-2 times, long-haired rabbit down fiber is opened separately for 1-2 times, and the two fibers are mixed and laid together for 3 times. , after adding the blending agent, beat it again; finally carry out bagging treatment; in terms of mass percentage, the blending agent includes 3% and hair oil FX-906, 1% antistatic agent FX-AS301, and 1% strengthening agent FX -VSE.
[0022] ...
PUM
| Property | Measurement | Unit |
|---|---|---|
| Fineness | aaaaa | aaaaa |
| Length | aaaaa | aaaaa |
| Fineness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More