Embodiment 1
[0038] The impact-resistant double-sided adhesive tape for display devices is produced by the following process: that is, the substrate layer is formed from a polyethylene terephthalate film with a thickness of 50 micrometers, and one side of the substrate layer is applied with a doctor blade Method: 100 parts by weight of acrylic resin mixture (polymerized by 100 parts by weight of n-butyl acrylate, 90 parts by weight of 2-ethylhexyl acrylate and 10 parts by weight of acrylic acid, with a weight average molecular weight of 700000), 1 A mixture of parts by weight of foaming agent (MSH-320 from SDI), 1 part by weight of curing agent (isocyanate) and 100 parts by weight of solvent (methyl ethyl ketone) is applied to a thickness of 90 microns and heated at 170°C. Foaming is carried out under the temperature condition of 100 microns to form a foaming adhesive layer with a thickness of 100 microns, and the acrylic resin mixture of 100 parts by weight (by 100 parts by weight of norma...
Embodiment 2
[0040] The impact-resistant double-sided adhesive tape for display equipment is produced by the following process: that is, the substrate layer is formed from a polyethylene terephthalate film with a thickness of 50 micrometers, and the two sides of the substrate layer are coated by a doctor blade method. By 100 parts by weight of acrylic resin mixture (polymerized by 100 parts by weight of n-butyl acrylate, 90 parts by weight of 2-ethylhexyl acrylate and 10 parts by weight of acrylic acid, the weight average molecular weight is 700000), 1 weight Parts of foaming agent (SDI MSH-320), 1 part by weight of curing agent (isocyanate) and 100 parts by weight of solvent (methyl ethyl ketone) are mixed and coated to a thickness of 90 microns at a temperature of 170 ° C The foaming was carried out under the following conditions to form a foamed adhesive layer with a thickness of 100 micrometers.
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |
| thickness | aaaaa | aaaaa |