Production process of antibacterial and warm-keeping quilt core
A production process and warm-keeping quilt technology, which is applied in the production process of warm-keeping quilt cores and in the field of antibacterial, can solve the problems of antibacterial quilt cores, poor warmth-keeping effect, and inability to process raw materials to meet demand, so as to achieve improved warmth-keeping effect and high process efficiency Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] A production process for an antibacterial and warm-keeping quilt core, comprising the following steps:
[0027] Step 1: Prepare cotton fiber, hemp fiber, carbon fiber, bamboo fiber, polyester fiber and polyacrylonitrile fiber for random inspection, and then weigh the raw materials according to the proportion;
[0028] Step 2: Mix the ingredients, put 40% of cotton fiber, 2% of hemp fiber, 4% of carbon fiber, 3% of bamboo fiber, 49% of polyester fiber and 2% of polyacrylonitrile fiber into the mixer, and set the temperature to 60°C , keep mixing for 60min;
[0029] Step 3: Use a cotton opener to open and disperse the cotton, and set the speed of the cotton opener to 500r / min until the mixed fiber material is evenly dispersed;
[0030] Step 4: Spread the dispersed mixed fibers with a carding machine and a web-laying machine, and set the speed at 1.5m / s;
[0031] Step 5: Use the filling machine to fill the mixed fiber, and seal the edge after filling;
[0032] Step 6: I...
Embodiment 2
[0035] A production process for an antibacterial and warm-keeping quilt core, comprising the following steps:
[0036] Step 1: Prepare cotton fiber, hemp fiber, carbon fiber, bamboo fiber, polyester fiber and polyacrylonitrile fiber for random inspection, and then weigh the raw materials according to the proportion;
[0037] Step 2: Mix the ingredients, put 45% of cotton fiber, 3% of hemp fiber, 5% of carbon fiber, 3% of bamboo fiber, 41% of polyester fiber and 3% of polyacrylonitrile fiber into the mixer, and set the temperature to 60°C , keep mixing for 60min;
[0038] Step 3: Use a cotton opener to open and disperse the cotton, and set the speed of the cotton opener to 500r / min until the mixed fiber material is evenly dispersed;
[0039] Step 4: Spread the dispersed mixed fibers with a carding machine and a web-laying machine, and set the speed at 1.5m / s;
[0040] Step 5: Use the filling machine to fill the mixed fiber, and seal the edge after filling;
[0041] Step 6: I...
Embodiment 3
[0044] A production process for an antibacterial and warm-keeping quilt core, comprising the following steps:
[0045] Step 1: Prepare cotton fiber, hemp fiber, carbon fiber, bamboo fiber, polyester fiber and polyacrylonitrile fiber for random inspection, and then weigh the raw materials according to the proportion;
[0046] Step 2: Mix the ingredients, put 50% of cotton fiber, 3% of hemp fiber, 6% of carbon fiber, 4% of bamboo fiber, 33% of polyester fiber and 4% of polyacrylonitrile fiber into the mixer, and set the temperature to 60°C , keep mixing for 30min;
[0047] Step 3: Use a cotton opener to open and disperse the cotton, and set the speed of the cotton opener to 500r / min until the mixed fiber material is evenly dispersed;
[0048] Step 4: Spread the dispersed mixed fibers with a carding machine and a web-laying machine, and set the speed at 1.5m / s;
[0049] Step 5: Use the filling machine to fill the mixed fiber, and seal the edge after filling;
[0050] Step 6: I...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction