A close-distance punching die with smooth punching surface
A close-range, punching surface technology, applied in the field of stamping die, can solve the problems of punching surface burr, easy to collapse, insufficient strength of inserts, etc., to avoid burrs and not easy to deform.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] see Figure 1 to Figure 6 , the figure shows a close-distance punching die with a smooth punching surface provided by Embodiment 1 of the present invention, including:
[0027] An upper mold mechanism 1, which includes an upper template 11, the bottom of the upper template 11 is provided with a first punch 12 and a second punch 13 arranged in parallel;
[0028] Lower mold mechanism 2, it comprises lower template 21, and workpiece is placed on lower template 21, and lower template 21 is provided with plunger 3, and plunger 3 comprises first plunger unit 31, second plunger unit 32 and the 3rd plunger Unit 33, one side of the second sub-unit 32 is spliced with the first sub-unit 31 to form the first blanking channel 4 corresponding to the first punch 12, the splicing surface of the second sub-unit 32 and the first sub-unit 31 It is a slope, the other side of the second sub-unit 32 is spliced with the third sub-unit 33 to form the second blanking channel 5 correspondin...
Embodiment 2
[0036] see Figure 1 to Figure 6 , the figure shows a close-distance punching die with a smooth blanking surface provided by Embodiment 2 of the present invention. On the basis of the above embodiments, this embodiment further makes the following technical solutions as improvements: the first A blanking channel 4 is sequentially provided with a first blanking part 41 and a second blanking part 42 from top to bottom, and the radial cross-sectional area of the first blanking part 41 is smaller than the radial cross-sectional area of the second blanking part 42; The first punch 12 is provided with a second stripping thimble 122 parallel to the first stripping thimble 121 , and the length of the second stripping thimble 122 is greater than the length of the first stripping thimble 121 .
[0037] In order to ensure the compressive strength of the second sub-unit, the diameter of the part formed by the punching edge in the middle of the second sub-unit gradually increases from t...
Embodiment 3
[0040] see Figure 1 to Figure 6 , the figure shows a close-distance punching die with a smooth blanking surface provided by Embodiment 3 of the present invention. On the basis of the above embodiments, this embodiment further makes the following technical solutions as improvements: the first The ends of the two stripping thimbles 122 are arc-shaped.
[0041] The end of the second stripping thimble is arc-shaped, and the contact area with the waste material is small, so as to avoid interfering with the rotation of the waste material.