The method for shortening the dyeing time when using Lanassin dye for non-red dyeing of cashmere
A technology of dyeing time and lanase, applied in the field of dyeing, can solve the problems of increased damage to dyed fibers, low production efficiency, large waste water discharge, etc. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] Example 1: The method for shortening the dyeing time when using Lanazine dye for cashmere red dyeing. In terms of fabric weight percentage, the following steps are included when the amount of Lanazine dye is less than or equal to 1%: Step A1: Heat the dye liquor to 25°C, then add acetic acid or formic acid to adjust the pH of the dye liquor to 4, based on the weight percentage of the fabric, and at the same time add 1.5% aliphatic amine polyoxyethylene ether anionic-nonionic surfactant, and then circulate for at least 10min; Step A2: with In terms of the weight percentage of the fabric, add no more than 1% of lanazol dye, then circulate for at least 10 minutes, then heat up to 80 °C at a rate of 0.5 °C / min, and keep the temperature for 40 minutes after the final temperature rise; Step A3: Rinse the fabric , after the rinsing is finished, the fabric is post-treated, and ammonia water is added to the treatment solution to make the pH of the treatment solution reach 7, base...
Embodiment 2
[0021] Example 2: The method for shortening the dyeing time when using Lanazine dye for cashmere red dyeing. In terms of fabric weight percentage, the following steps are included when the amount of Lanazine dye is less than or equal to 1%: Step A1: Heat the dye liquor to 35 ° C, then add acetic acid or formic acid to adjust the pH of the dye liquor to 6.5, in terms of fabric weight percentage, simultaneously add 2.0% aliphatic amine polyoxyethylene ether anion-nonionic surfactant, then circulate at least 10min; Step A2 : Based on the weight percentage of the fabric, add no more than 1% of Lanazine dye, then circulate for at least 10 minutes, then heat up to 99°C at a rate of 1.5°C / min, and keep the temperature for 50 minutes after the final temperature rise; Step A3: to The fabric is rinsed, and after the rinsing, the fabric is post-treated, and ammonia water is added to the treatment solution to make the pH of the treatment solution reach 8, based on the weight percentage of ...
Embodiment 3
[0022] Example 3: The method for shortening the dyeing time when using the Lannasin dye for cashmere red dyeing. In terms of the weight percentage of the fabric, when the amount of Lannasin dye is less than or equal to 1%, the following steps are included: Step A1: Heat the dye solution to 30°C, then add acetic acid or formic acid to adjust the pH of the dye liquor to 5, based on the weight percentage of the fabric, and add 1.6% aliphatic amine polyoxyethylene ether anionic-nonionic surfactant at the same time, and then circulate for at least 10min; Step A2: with In terms of the weight percentage of the fabric, add no more than 1% of Lanazine dye, then circulate for at least 10 minutes, then heat up to 90 °C at a rate of 1 °C / min, and keep the temperature for 45 minutes after the final temperature rise; Step A3: Rinse the fabric , after rinsing, the fabric is post-treated, and ammonia water is added to the treatment solution to make the pH of the treatment solution reach 7.5, b...
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com