A kind of desulfurizer for gas well of Maokou Formation and preparation method thereof
A technology for desulfurization agent and gas well, which is applied in the direction of gas fuel, recycling technology, plastic recycling, etc., can solve the problem of desulfurization efficiency reduction of desulfurizer, and achieve the effect of simple and easy to control preparation method, suitable for popularization and application, and good desulfurization effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] A desulfurizer for a well in the Maokou Formation is weighed according to the following weights:
[0028] Polymer porous microspheres 22kg, nonionic surfactant 5kg, zinc oxide 60kg, graphene oxide 5kg, pre-gelatinized starch 6kg, hydrophobic agent 2kg.
[0029] The preparation method of the above-mentioned desulfurization agent for the gas well of the Maokou Formation is as follows:
[0030] (1) Put the pre-gelatinized starch into the mixing tank, add water under the stirring conditions of 1300r / min, the weight ratio of the pre-gelatinized starch to the water is 2:20, mix well, and obtain the mixing liquid I.;
[0031] (2) Put zinc oxide into the mixture I. Increase the stirring speed to 2000r / min, stir for 25min, and then put graphene oxide, nonionic surfactants and hydrophobic agents into the mixing tank, continue to stir for 35min, and obtain the mixture II.;
[0032] (3) Put polymer porous microspheres into the mixed liquid II. and stir it for 70min under the condition of...
Embodiment 2
[0035] A desulfurizer for a well in the Maokou Formation is weighed according to the following weights:
[0036] Polymer porous microspheres 20kg, nonionic surfactant 3kg, zinc oxide 65kg, graphene oxide 4kg, pre-gelatinized starch 5kg, hydrophobic agent 3kg.
[0037] The preparation method of the above-mentioned desulfurization agent for the gas well of the Maokou Formation is as follows:
[0038] (1) Put the pre-gelatinized starch into the mixing tank, add water under the stirring conditions of 1500r / min, the weight ratio of the pre-gelatinized starch to the water is 1:20, mix well, and obtain the mixing liquid I.;
[0039] (2) Put zinc oxide into the mixture I., increase the stirring speed to 2000r / min, stir for 30min, and then put graphene oxide, nonionic surfactant and hydrophobic agent into the mixing tank, continue to stir for 30min, and obtain the mixture II.;
[0040] (3) Add polymer porous microspheres to the mixture II., stir for 80min under the condition of 500r / min, a...
Embodiment 3
[0043] A desulfurizer for a well in the Maokou Formation is weighed according to the following weights:
[0044] Polymer porous microspheres 24kg, nonionic surfactant 7kg, zinc oxide 55kg, graphene oxide 6kg, pre-gelatinized starch 7kg, hydrophobic agent 1kg.
[0045] The preparation method of the above-mentioned desulfurization agent for the gas well of the Maokou Formation is as follows:
[0046] (1) Put the pre-gelatinized starch into the mixing tank, add water under the stirring conditions of 1000r / min, the weight ratio of the pre-gelatinized starch to the water is 3:20, mix well, and obtain the mixing liquid I.;
[0047] (2) Put zinc oxide into the mixture I., increase the stirring speed to 2000r / min, stir for 20min, and then put graphene oxide, nonionic surfactants and hydrophobic agents into the mixing tank, continue to stir for 40min, and obtain the mixed liquid II.;
[0048] (3) Put polymer porous microspheres into the mixture II., stir for 60min under the condition of 300r...