Process for producing absorption styptic sponge used in operation
A production process and absorbency technology, which is applied in the new process field of producing surgical absorbent hemostatic sponge with animal leather, can solve the problems of inconvenient use
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Step 1, with 10% Ca(OH) 2 Soak the washed animal leather dregs in an aqueous solution for 70 days to make expanded leather;
[0019] Step 2, after the swollen leather is washed with water of ph=6.5, the molar concentration is [H + ]=0.45(±1)mol / l, HCl, H mixed in a ratio of 4:6 2 SO 4 The solution is soaked until the pigment on the leather can be rubbed off, and the leather fiber is further expanded to facilitate the complete removal of harmful ingredients;
[0020] Step 3, adding NaOH to the soaking solution in Step 2, neutralizing the soaking solution to a pH value of 6.5, then mechanically stirring the leather in the soaking tank for 4 days to make a neutral leather;
[0021] Step 4: After washing the neutral leather with water, immerse in 6% HCl aqueous solution for 5 days, then dilute the HCl aqueous solution with water to a pH value of 5 to make the fibers in the leather more swollen Swell, forming colloidal leather;
[0022] Step 5: Add NaOH to the soaking s...
Embodiment 2
[0030] Step 1, with 8% Ca(OH) 2 Soak the washed animal leather dregs in an aqueous solution for 80 days to make expanded leather;
[0031] Step 2, after the swollen leather is washed with water of ph=6.5, the molar concentration is [H + ]=0.45(±1)mol / l, HCl, H mixed in a ratio of 5:5 2 SO 4 The solution is soaked until the pigment on the leather can be rubbed off, and the leather fiber is further expanded to facilitate the complete removal of harmful ingredients;
[0032] Step 3, adding NaOH to the soaking solution in Step 2, neutralizing the soaking solution to a pH value of 6.5, then mechanically stirring the leather in the soaking tank for 6 days to make a neutral leather;
[0033] Step 4: After washing the neutral leather with water, immerse in 6% HCl aqueous solution for 5 days, then dilute the HCl aqueous solution with water to a pH value of 5 to make the fibers in the leather more swollen Swell, forming colloidal leather;
[0034] Step 5: Add NaOH to the soaking so...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com