Tempering ceramic glaze paint

A technology of tempering porcelain and enamel, applied in coating and other directions, can solve the problems of excessive manpower and material resources, waste of time and money, inability to re-fire and other problems, and achieve the effect of strong stain resistance, strong corrosion resistance and low price.

Inactive Publication Date: 2009-08-26
王剑
View PDF3 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

But with the passage of time, the sun exposure and the pollution of the atmospheric environment, the tiles become old and cracked and lose their original color and luster, especially the exterior walls eroded by acid rain and sea breeze are full of spots, seriously affecting the appearance and city appearance. cityscape
But the tiles and buildings are combined and cannot be refired
Because the surface of tiles is very smooth, it is difficult for general paint and paint to adhere to the surface for a long time, so the method of brushing paint cannot solve the problem
If the old tiles are smashed and reinstalled, it will require a lot of manpower and material resources, waste time and money, and cause great inconvenience to the surrounding environment and traffic

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Tempering ceramic glaze paint

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0021] Hydroxy-containing acrylic resin (brand AH2870) 43

[0022] Inorganic ceramic pigments 15

[0023] Acrylate type leveling agent (MFAOH) 4

[0024] Defoamer: Defoaming polysiloxane solution 861 2

[0025] Anti-sedimentation agent: HFGEL series organic bentonite variable additive type 140 3

[0026] Adhesion Promoter: Silane (KEPER993) 7

[0027] Dispersant: Zinc Stearate 8

[0028] Filler: titanium dioxide 10

Embodiment 2

[0030] Hydroxyl-containing acrylic resin (brand AH2870) 40

[0031] Inorganic ceramic pigments 10

[0032] Leveling agent: wax powder (DE8418) 3

[0033] Defoamer: CFC-2000 0.5

[0034] Anti-sedimentation agent: HFGEL series organic bentonite variable additive type 160 1

[0035] Adhesion promoter: silane (KEPER993) 5

[0036] Dispersant: aluminum stearate 5

[0037] Filler: calcium carbonate 5

Embodiment 3

[0039] Hydroxy-containing acrylic resin (brand AH2870) 45

[0040] Inorganic ceramic pigments 20

[0041] Leveling agent: special modified reactive polysiloxane (DE2890) 5

[0042] Antifoaming agent: calcium stearate 5

[0043] Anti-settling agent: polyamide anti-sag (CIMA240-20) 5

[0044] Adhesion promoter: silane (KEPER993) 10

[0045] Dispersant: barium stearate 9

[0046] Filler: alumina powder 12

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The tempered enamel paint is characterized in that, in terms of weight percentage, it consists of: 40-45 hydroxyl-containing acrylic resin, 10-20 inorganic ceramic pigment, 2-5 leveling agent, 0.5-5 defoaming agent, and 0.5-5 anti-settling agent , Adhesion promoter 5-10, dispersant 5-10, filler 5-15. The invention is simple in construction, can be painted with a brush or sprayed with ordinary spraying equipment, and has the roundness, smoothness, firmness, corrosion resistance and other properties of enamel. After many tests, there is no abnormal change in the range of low temperature resistance -40 ℃ ~ high temperature resistance 160 ℃; water resistance 268 hours without abnormality; alkali resistance 168 hours without abnormality; washing resistance ≥ 2000 times; artificial weather aging resistance 1000 hours No blistering, no peeling, no cracks; no obstacles in the construction of the second coat of brushing; the coating is resistant to temperature denaturation for 5 cycles without abnormalities. The price of this product is low, and its service life can reach more than 10 years.

Description

technical field [0001] The invention belongs to the field of coatings, in particular to a tempered enamel paint. Background technique [0002] Ceramic tiles are mainly used for decoration and protection of the inner and outer walls of buildings. The surface of ceramic tile glaze is smooth, bright in color and strong in corrosion resistance. But with the passage of time, the sun exposure and the pollution of the atmospheric environment, the tiles become old and cracked and lose their original color and luster, especially the exterior walls eroded by acid rain and sea breeze are full of spots, seriously affecting the appearance and city appearance. City appearance. But the tiles and buildings are combined and cannot be refired. Because the surface of the ceramic tile is very smooth, it is difficult for general paint and paint to adhere to the surface for a long time, so the method of brushing paint cannot solve the problem. If the old tiles are smashed and reinstalled, it w...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine