[0012] Example 1: Weigh 25 kg of behenyl alcohol, 35 kg of behenic acid saturated alkyd, 15 kg of stearyl alcohol, 5 kg of ethylene glycol saturated amide, 5 kg of ethylene glycol methyl ether, 5 kg of methyl silicone oil, and 2 kg of azobenzene. Put it into a heating pot, heat to 200°C, and stir continuously for 18 hours, then put the mixture into the ice bank, freeze at 0°C for 4 hours, take it out for crushing and granulation. After granulation, add 8 kg of silicon dioxide, mix evenly, and then stamp it into small flakes with 1.5 grams per grain, and pack it into plates.
example 2
[0013] Example 2: Weigh 22 kg of behenyl alcohol, 38 kg of behenic acid saturated alkyd, 19 kg of stearyl alcohol, 4 kg of ethylene glycol saturated amide, 4 kg of ethylene glycol methyl ether, 7 kg of methyl silicone oil, and 1 kg of azobenzene. Put it into a heating pot, heat it to 160°C, and stir continuously for 20 hours, then put the mixture into the freezer, freeze it at 1°C for 5 hours, take it out for pulverization and granulation. After granulation, add 5kg of silicon dioxide, mix evenly, and then stamp it into small flakes with 1.5 grams per grain, and pack it into plates.
example 3
[0014] Example 3: Weigh 28 kg of behenyl alcohol, 32 kg of behenic acid saturated alkyd, 12 kg of stearyl alcohol, 7 kg of ethylene glycol saturated amide, 7 kg of ethylene glycol methyl ether, 3 kg of methyl silicone oil, and 3 kg of azobenzene, and put them together Put it into a heating pot, heat it to 250°C, and stir continuously for 15 hours, then put the mixture into a freezer, freeze at -1°C for 3 hours, take it out for crushing and granulation. After granulation, add 8 kg of silicon dioxide, mix evenly, and then stamp it into small flakes with 1.5 grams per grain, and pack it into plates.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com