Prescription of decolorant for charging barrel of plastics processing machine and method of producing the same
A technology for processing machinery and manufacturing methods, which is applied in the formulation and manufacturing of barrel decolorizers, can solve the problems of waste of raw materials and electric energy, low cleaning efficiency, etc., and achieve the effect of saving costs
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0043] Embodiment one, the raw material formula and weight of use are: 18 parts of T-10 or fatty alcohols or alkylphenols as surfactant, 20 parts of ethanol or Virahol or mixed propanol or mixed butanol or n-butanol Or methanol or isobutanol as alcohol solvent, 18 parts of dibutyl phthalate or dioctyl phthalate or dibutyl sebacate or dioctyl sebacate or dioctyl adipate or Diisooctyl phthalate or dicarboxylic acid phthalate or glycerol triacetate or butyl epoxy fatty acid as plasticizer, use 44 parts of water as dilution. Its production process is as follows:
[0044] 1. Dilute one of the above-mentioned surfactants (i.e. 18 parts of T-10 or fatty alcohols or alkylphenols) with an appropriate amount of water (some surfactants, such as T-10, are diluted It must be heated to 30-60 degrees Celsius to facilitate the dissolution of the surfactant) and then poured into the reaction kettle;
[0045] 2. Add one of the above-mentioned plasticizers into the reactor (that is, 18 parts o...
Embodiment 2
[0048] Embodiment two, the raw material formula and weight used are: 16 parts of dioctyl phthalate as plasticizer, 8 parts of ethanol and 8 parts of isopropanol as alcohol solvent, 16 parts of T-10 as surfactant, Add 4 parts of phosphoric acid, 8 parts of ethylene glycol monobutyl ether as an ether solvent, 10 parts of 6501—a detergent aid, and use 30 parts of water for dilution. Its production process is as follows:
[0049] 1. Pour 4 parts of phosphoric acid into the reaction kettle, add an appropriate amount of water to dilute the phosphoric acid;
[0050] 2. Dilute 16 parts of surfactant - T-10 with water (heat the water to 30-60 degrees Celsius when diluting) and pour it into the reaction kettle;
[0051] 3. Add 16 parts of dioctyl phthalate into the reactor and stir, while controlling the temperature in the reactor at 15-25 degrees Celsius for 30 minutes;
[0052] 4. Dilute 10 parts of washing aid - 6501 with an appropriate amount of water and mix it with 8 parts of et...
Embodiment 3
[0057] Embodiment 3, a formula of a decolorizing agent for a barrel of a plastic processing machine, the weight percentages of each material are respectively: surfactant accounts for 3%, alcohol solvent accounts for 3%, plasticizer accounts for 3%, and the rest is water .