Process for continuously producing solid salt from salt solution
A salt solution and solid salt technology, applied in the direction of alkali metal chloride, energy input, etc., can solve the problems of high energy consumption, heat short-circuit cycle, large floor area, etc., and achieve the effect of low energy consumption and no pollution to the environment
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] A process for continuously producing solid salt using salt solution, comprising the following steps:
[0014] First, the salt solution with a pressure of 0.1mpa and a salt content of 8% is sent into the dispersion chamber, so that the salt solution is subjected to a pressure of 0.5mpa when passing through the dispersion chamber, and the salt solution is dispersed into a volume less than or equal to 15 cubic millimeters under this pressure The particulate water droplets enter the salt-forming chamber;
[0015] Second, the air with a pressure of 0.1mpa, a temperature of 10°C, and a speed of 1m / s is input into the heater for heat treatment. The heating temperature is 50°C, and the heating time is 10 seconds. The heated air flows from at least two directions. Enter the salt forming chamber, make the air cross flow and mix with the dispersed salt solution;
[0016] Thirdly, heat the mixture obtained in the salt forming chamber in the previous step to evaporate water, contro...
Embodiment 2
[0021] A process for continuously producing solid salt using salt solution, comprising the following steps:
[0022] First, a salt solution with a pressure of 0.5mpa and a salt content of 20% is sent into the dispersion chamber, so that the salt solution is subjected to a pressure of 3mpa when passing through the dispersion chamber, and the salt solution is dispersed into a volume less than or equal to 15 cubic millimeters under this pressure Particle water drops enter the salt forming chamber;
[0023] Second, the air with a pressure of 3mpa, a temperature of 20°C, and a speed of 5m / s is fed into the heater for heat treatment. The heating temperature is 60°C and the heating time is 10 seconds. The heated air flows from at least two directions. Enter the salt forming chamber, make the air cross flow and mix with the dispersed salt solution;
[0024] Third, the mixture obtained in the salt-forming chamber in the previous step is heated to evaporate water, and the temperature i...
Embodiment 3
[0029] A process for continuously producing solid salt using salt solution, comprising the following steps:
[0030] First, the salt solution with a pressure of 5mpa and a salt content of 40% is sent into the dispersion chamber, so that the salt solution is subjected to a pressure of 5mpa when passing through the dispersion chamber, and the salt solution is dispersed into particles with a volume less than or equal to 15 cubic millimeters under this pressure After the water drops enter the salt forming chamber;
[0031] Second, the air with a pressure of 5mpa, a temperature of 30°C, and a speed of 10m / s is input into the heater for heat treatment. The heating temperature is 80°C, and the heating time is 5 seconds. The heated air enters from at least two directions Salt-forming chamber, allowing the air to flow across each other to mix with the dispersed salt solution;
[0032] Third, the mixture obtained in the salt-forming chamber in the previous step is heated to evaporate w...