Anti-corrosive treatment method of welded junction part of construction process pipe of heavy caliber push pipe
A technology of construction technology and treatment method, which is applied in the direction of pretreatment surface, device for coating liquid on the surface, coating, etc., which can solve the problems of poor construction technology performance, huge equipment, tools and power equipment, and low solid content.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0089] A method for anti-corrosion treatment of welding joints of pipelines in large-diameter pipe jacking construction technology, which specifically applies open excavation construction or pipe jacking construction technology for pipeline installation; The spaces are fixed together by welding; the outside of the pipeline is provided with a sacrificial anode protection device 3 fixedly connected to the outer wall of the pipeline, and the entire outside of the pipeline is provided with a protective coating;
[0090] The sacrificial anode protection device 3 is made of magnesium alloy or zinc alloy; the specific requirements meet the "4 Technical Conditions" in "The People's Republic of China Petroleum and Natural Gas Industry Standards. Design Specifications for Sacrificial Anode Cathodic Protection of Buried Steel Pipelines" SY / T0019-97 Provisions.
[0091] The anti-corrosion treatment method for the welding joints of pipelines in the large-diameter pipe jacking construction ...
Embodiment 2
[0107] The anti-corrosion treatment method for the welding joints of large-diameter pipe jacking construction technology uses open excavation construction or pipe jacking construction technology for pipeline installation; the process pipeline is a pipeline for pipe jacking construction in sections, and the welding method is used between each section fixed together; the outside of the pipeline is provided with a sacrificial anode protection device 3 fixedly connected to the outer wall of the pipeline, and the entire pipeline is provided with a protective coating; it is characterized in that:
[0108] The anti-corrosion treatment method for the welding joints of pipelines in the large-diameter pipe jacking construction process specifically uses a solvent-free liquid epoxy coating to quickly repair the coating at the welding joints on the outer wall of the pipeline so as to quickly form an integral protective coating on the outside of the pipeline , the coating properties of the s...
PUM
Property | Measurement | Unit |
---|---|---|
wear resistance | aaaaa | aaaaa |
dielectric strength | aaaaa | aaaaa |
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com