Method for producing color display tube
A production method and color display technology, which is applied in the field of color display tubes, can solve the problem that the qualified rate of screen making is only 20%, and achieve the effects of reducing production costs and improving production efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A method for producing a color display tube includes a photosensitive glue coating process, a black matrix coating process, a phosphor coating process, an organic film coating process, an aluminum steaming process, and a baking process. In the film coating step, a protective layer coating step is provided.
[0018] The protective film coating process is:
[0019] a. Filter the ethanol solution of ethyl orthosilicate with a pH value of 3.5 and a volume concentration of 3.5% adjusted with phosphoric acid (GB1282-77) through a 240-mesh silk cloth, and then pour it on the screen, shake it evenly to make the solution uniform Distributed on the black bottom layer and the inner surface of the screen;
[0020] b. Install the screen of the coated display screen down to the centrifuge fixture, and centrifuge and dry for 6 minutes at 450 rpm to make the protective layer coating liquid evenly spin-coated on the display tube screen Inside.
[0021] c. Keep the centrifuged display at 115℃ ...
Embodiment 2
[0023] A method for producing a color display tube includes a photosensitive glue coating process, a black matrix coating process, a phosphor coating process, an organic film coating process, an aluminum steaming process, and a baking process. In the film coating step, a protective layer coating step is provided.
[0024] The protective film coating process is:
[0025] a. Filter the ethanol solution of ethyl orthosilicate with a pH of 3.6 and a volume concentration of 4% adjusted by phosphoric acid (GB1282-77) through 200 mesh silk cloth, and then pour it on the screen, shake it evenly to make the solution uniform Distributed on the black bottom layer and the inner surface of the screen;
[0026] b. Install the screen of the coated display screen down to the centrifuge fixture, and centrifuge for 6 minutes at 500rpm to make the protective layer coating liquid evenly spin-coated in the display tube screen .
[0027] c. Keep the centrifuged display at 120°C for 62 minutes to harden t...
Embodiment 3
[0029] A method for producing a color display tube includes a photosensitive glue coating process, a black matrix coating process, a phosphor coating process, an organic film coating process, an aluminum steaming process, and a baking process. In the film coating step, a protective layer coating step is provided.
[0030] The protective film coating process is:
[0031] a. Filter the ethanol solution of ethyl orthosilicate with a pH of 3.8 and a volume concentration of 4.5% adjusted with phosphoric acid (GB1282-77) through 240 mesh silk cloth, and then pour it on the screen, shake it evenly to make the solution uniform Distributed on the black bottom layer and the inner surface of the screen;
[0032] b. Install the screen of the coated display screen down to the centrifuge fixture, and centrifuge for 5 minutes at a speed of 550 rpm to make the protective layer coating liquid evenly spin-coated on the display tube screen .
[0033] c. Keep the centrifuged display at 125℃ for 60 minu...