Method for synthesizing high molecular retanning dyeing auxiliary agents through enzyme catalysis
A technology for synthesizing polymers and dyeing auxiliaries, which is applied in dyeing, chemical treatment of small raw hide/large raw hide/leather skin/fur, textiles and papermaking, etc., to achieve the effect of fine grain, high absorption rate and good permeability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0007] Example 1: Dissolve 8 grams of 2,3-dihydroxynaphthalene-6-sodium sulfonate and 5.3 grams of p-aminobenzenesulfonic acid in 32 grams of deionized water, mix well and heat to 30°C, then neutralize the system with sodium bicarbonate When the pH reaches 7.6, add 3 ml of HRP solution with a concentration of 0.5 g / L, then add 6.8 g of hydrogen peroxide solution with a mass fraction of 30%, and control the dropping time for 1.5 hours. After the addition, continue to keep warm at 30°C React for 3 hours to get the polymer retanning and dyeing auxiliaries.
Embodiment 2
[0008] Example 2: Dissolve 9 grams of 2,3-dihydroxynaphthalene-6-sodium sulfonate and 4.2 grams of p-aminobenzenesulfonic acid in 36 grams of deionized water, mix well and heat to 30°C, then neutralize the system with sodium bicarbonate When the pH reaches 7.4, add 4 ml of HRP solution with a concentration of 0.5 g / L, and then add 6.2 g of hydrogen peroxide solution with a mass fraction of 30% dropwise, and control the dropping time for 1.8 hours. After the addition, continue to keep warm at 30°C React for 2.5 hours to get the polymer retanning and dyeing auxiliaries.
Embodiment 3
[0009] Example 3: Dissolve 10 grams of 2,3-dihydroxynaphthalene-6-sodium sulfonate and 3.3 grams of p-aminobenzenesulfonic acid in 38 grams of deionized water, mix well and heat to 30°C, then neutralize the system with sodium bicarbonate When the pH reaches 7.8, add 5 ml of HRP solution with a concentration of 0.5 g / L, and then dropwise add 7 g of hydrogen peroxide solution with a mass fraction of 30%, and control the dropping time for 1.5 hours. After the addition, continue to keep warm at 30°C React for 2.8 hours to obtain polymer retanning and dyeing auxiliaries.
PUM
Property | Measurement | Unit |
---|---|---|
quality score | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com