A technology of wool knitted fabrics and finishing agents, which is applied in textiles and papermaking, fiber treatment, animal fibers, etc., can solve the problems of high processing temperature of finishing agents, poor shape memory finishing effect, etc. The risk of small color changes, the effect of simple processing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0081] 250g of polyoxypropylene triol (Mw=3000), 50g of polyoxyethylene diol (Mw=1000) was dried by vacuum heating, and then mixed with 59g of hexamethylene diisocyanate (HDI), and reacted at 88-92°C for 3 hour, then add 40 g of ethyl acetate and cool to obtain a prepolymer solution. Then 500 milliliters of mixed solvent ethanol / isopropanol (volume ratio is 8 / 2) and 150 g of 25% sodium bisulfite aqueous solution are added, and at the same time vigorously stirred; after 1 hour, add a little 10% hydrochloric acid solution to adjust When the pH value reaches 4-5, it is diluted with water to obtain a translucent polyurethane composite aqueous solution containing 40% solid content.
Embodiment 2
[0083] 120g PO / EO polyether polyol (Mw=5000, hydroxyl value 33mgKOH / g), 50g polyoxyethylene diol (Mw=1000), 5g polydimethylsiloxane diol (Mw=1800, BY16 -201, DowCorning Toray), and 42g of isophorone diisocyanate, reacted at 90-95°C for 2 hours, then cooled; add 250ml of ethanol, mix well, and add a 20% sodium bisulfite aqueous solution while stirring 115g, reacted at room temperature to 40°C for 1.5 hours, the reactant changed from milky white to translucent. Add 10% hydrochloric acid solution to adjust the pH value to 5-6, and then add water to dilute to obtain a polyurethane aqueous solution with a solid content of 40%.
Embodiment 3
[0085] Put 400g polyoxyethylene-polyoxypropylene triol (Mw=3000), 100g polycaprolactone diol (PCL, Mw=2000), and 90g 1,6-hexamethylene diisocyanate at 90~110℃ React for 2.5 hours, cool to below 40°C, add ethanol / isopropanol mixed solvent (volume ratio is 8 / 2) 800ml, and 250g 25% sodium bisulfite aqueous solution, stir for 1.5 hours, then add 9g p-toluenesulfonic acid, Dilute with water to obtain a polyurethane emulsion with a solid content of 30%.
PUM
Property | Measurement | Unit |
---|---|---|
Functional group degree | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com